MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Bynel® 41E871 Anhydride Modified LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins.

BYNEL 41E871 is a grade with a medium-high level of anhydride modification, and is mainly intended for use as a component in a blend with other polyolefin resins.

Physical properties of BYNEL Series 4100 resins are typical of linear low-density polyethylene resins with similar density and melt index values. Use of these adhesive resins in coextruded PE/barrier structures offers improved thermal resistance over that of ethylene vinyl acetate-based adhesive resins.

BYNEL 4100 series resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE and ethylene copolymers. Series 4100 resins can be used in coextrusion processes including:

  • blown film
  • cast film/sheet
  • blow molding
  • melt and solid phase thermoforming
  • sheet and tubing

LLDPE resins are known for their temperature resistance, clarity and toughness, which make the 4100 series resins work well in applications such as:

  • boil-in-bag structures
  • blow molded containers in which drop strength is important
  • bag-in-box films
  • film where LLDPE is the heat seal layer.

BYNEL 41E871 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlayers in composite packages for food use. This regulation describes adhesives that may be safely used as components of articles intended for use in packaging, transporting or holding food. This regulation requires that either (1) the adhesive is separated from the food by a functional barrier, or (2) the quantity of adhesive which contacts fatty or aqueous foods does not exceed the trace amounts at the seams or edges. Customers should satisfy themselves that the food contact material is serving as a functional barrier to the adhesive.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792, ISO 1183
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 106 °C223 °FFreezing Point; ASTM D3418
 121 °C250 °FASTM D3418, ISO 3146
Vicat Softening Point 100 °C212 °FASTM D1525, ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 260 °C<= 500 °F
Feed Temperature 160 °C320 °FCoExtrusion with EVOH Processing
 160 °C320 °FCoExtrusion with Nylon Processing
Zone 2 185 °C365 °FCoExtrusion with EVOH Processing
 185 °C365 °FCoExtrusion with Nylon Processing
Zone 3 235 °C455 °FCoExtrusion with EVOH Processing
 235 °C455 °FCoExtrusion with Nylon Processing
Zone 4 235 °C455 °FCoExtrusion with EVOH Processing
 260 °C500 °FCoExtrusion with Nylon Processing
Zone 5 235 °C455 °FCoExtrusion with EVOH Processing
 260 °C500 °FCoExtrusion with Nylon Processing
Adapter Temperature 235 °C455 °FCoExtrusion with EVOH Processing
 260 °C500 °FCoExtrusion with Nylon Processing
Die Temperature 235 °C455 °FCoExtrusion with EVOH Processing
 260 °C500 °FCoExtrusion with Nylon Processing
Melt Temperature 210 - 235 °C410 - 455 °FCoExtrusion with EVOH Processing
 <= 260 °C<= 500 °FCoExtrusion with Nylon Processing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Bynel® 41E755 Anhydride Modified LLDPE
Dow Bynel® 41E710 Anhydride Modified LLDPE
Dow Bynel® 42E703 Adhesive Resin
Westlake EM1870AA Low Density Polyethylene
Dow Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin

PDTA4930 / 170370

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.