MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.22 - 1.76 g/cc0.0439 - 0.0636 lb/in³Average value: 1.49 g/cc Grade Count:42
Filler Content 10.0 - 40.0 %10.0 - 40.0 %Average value: 23.8 % Grade Count:8
Water Absorption 0.0700 - 0.100 %0.0700 - 0.100 %Average value: 0.0744 % Grade Count:9
Moisture Absorption at Equilibrium 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.155 % Grade Count:6
Linear Mold Shrinkage 0.000 - 0.0400 cm/cm0.000 - 0.0400 in/inAverage value: 0.00620 cm/cm Grade Count:25
Linear Mold Shrinkage, Transverse 0.00500 - 0.0220 cm/cm0.00500 - 0.0220 in/inAverage value: 0.00900 cm/cm Grade Count:7
Melt Flow 5.00 - 26.0 g/10 min5.00 - 26.0 g/10 minAverage value: 15.0 g/10 min Grade Count:6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115 - 119115 - 119Average value: 117 Grade Count:10
Tensile Strength, Ultimate 29.0 - 153 MPa4210 - 22200 psiAverage value: 101 MPa Grade Count:40
Tensile Strength, Yield 38.0 - 114 MPa5510 - 16500 psiAverage value: 74.8 MPa Grade Count:6
Elongation at Break 1.10 - 247 %1.10 - 247 %Average value: 16.2 % Grade Count:38
Modulus of Elasticity 1.76 - 10.7 GPa256 - 1550 ksiAverage value: 6.65 GPa Grade Count:16
Flexural Yield Strength 47.0 - 210 MPa6820 - 30500 psiAverage value: 152 MPa Grade Count:42
Flexural Modulus 1.67 - 15.5 GPa243 - 2250 ksiAverage value: 7.20 GPa Grade Count:41
Izod Impact, Notched 0.491 - 52.9 J/cm0.920 - 99.0 ft-lb/inAverage value: 3.42 J/cm Grade Count:23
 1.6017 - 1.6017 J/cm
@Temperature -28.9 - -28.9 °C
3.0006 - 3.0006 ft-lb/in
@Temperature -20.0 - -20.0 °F
Average value: 1.60 J/cm Grade Count:1
Izod Impact, Unnotched 5.34 - 10.7 J/cm10.0 - 20.0 ft-lb/inAverage value: 7.48 J/cm Grade Count:12
Izod Impact, Notched (ISO) 5.00 kJ/m² - NB2.38 ft-lb/in² - NBAverage value: 9.10 kJ/m² Grade Count:8
Charpy Impact Unnotched 2.20 J/cm² - NB10.5 ft-lb/in² - NBAverage value: 3.93 J/cm² Grade Count:5
 2.20 J/cm² - NB
@Temperature -30.0 - -30.0 °C
10.5 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 3.47 J/cm² Grade Count:5
Charpy Impact, Notched 0.390 - 8.00 J/cm²1.86 - 38.1 ft-lb/in²Average value: 1.00 J/cm² Grade Count:21
 0.400 - 1.90 J/cm²
@Temperature -30.0 - -30.0 °C
1.90 - 9.04 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.938 J/cm² Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+11 - 1.20e+17 ohm-cm2.00e+11 - 1.20e+17 ohm-cmAverage value: 1.99e+16 ohm-cm Grade Count:23
Surface Resistance 2.00e+10 - 4.00e+17 ohm2.00e+10 - 4.00e+17 ohmAverage value: 8.15e+16 ohm Grade Count:13
Dielectric Constant 2.80 - 4.302.80 - 4.30Average value: 3.63 Grade Count:7
Dielectric Strength 16.5 - 32.0 kV/mm420 - 813 kV/inAverage value: 23.1 kV/mm Grade Count:15
Dissipation Factor 0.00330 - 0.02400.00330 - 0.0240Average value: 0.0155 Grade Count:7
Arc Resistance 87.0 - 129 sec87.0 - 129 secAverage value: 107 sec Grade Count:4
Comparative Tracking Index 175 - 600 V175 - 600 VAverage value: 309 V Grade Count:10
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 130 µm/m-°C11.1 - 72.2 µin/in-°FAverage value: 37.6 µm/m-°C Grade Count:14
CTE, linear, Transverse to Flow 35.0 - 116 µm/m-°C19.4 - 64.4 µin/in-°FAverage value: 76.6 µm/m-°C Grade Count:12
Melting Point 210 - 225 °C410 - 437 °FAverage value: 223 °C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 86.0 - 228 °C187 - 442 °FAverage value: 198 °C Grade Count:23
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 211 °C120 - 412 °FAverage value: 176 °C Grade Count:39
Glass Transition Temp, Tg 20.0 - 71.0 °C68.0 - 160 °FAverage value: 52.8 °C Grade Count:4
Flammability, UL94 HB - V-0HB - V-0Grade Count:34
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 260 °C68.0 - 500 °FAverage value: 176 °C Grade Count:20
Die Temperature 240 - 260 °C464 - 500 °FAverage value: 254 °C Grade Count:8
Melt Temperature 230 - 270 °C446 - 518 °FAverage value: 247 °C Grade Count:14
Mold Temperature 30.0 - 107 °C86.0 - 225 °FAverage value: 84.3 °C Grade Count:16
Drying Temperature 116 - 130 °C240 - 266 °FAverage value: 123 °C Grade Count:9
Moisture Content 0.0200 %0.0200 %Average value: 0.0200 % Grade Count:5
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 84.4 MPa Grade Count:9
Vent Depth 0.00127 cm0.000500 inAverage value: 0.00127 cm Grade Count:3
Hot-Working Temperature 250 - 260 °C482 - 500 °FAverage value: 255 °C Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled

O3219 / 78177

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.