MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Vectra® C130 Liquid Crystal Polymer (LCP), 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes:

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ISO 1183
Water Absorption 0.020 %0.020 %Immersion to equilibrium; ISO 62
Moisture Absorption at Equilibrium 0.020 %0.020 %ISO 62
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in
Linear Mold Shrinkage, Transverse 0.0020 cm/cm0.0020 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 160 MPa23200 psiISO 527
Elongation at Break 1.9 %1.9 %IEC 527
Tensile Modulus 15.0 GPa2180 ksiISO 527
Flexural Strength 245 MPa35500 psiISO 178
Flexural Modulus 14.0 GPa2030 ksiISO 178
Compressive Strength 139 MPa20200 psi1% Deflection, ISO 604
Compressive Modulus 22.0 GPa3190 ksiISO 604
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²ISO 179
Tensile Impact Strength 70.0 kJ/m²33.3 ft-lb/in²Notched; ASTM D1822
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 93
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 93
Dielectric Constant  3.4
@Frequency 1e+7 Hz
3.4
@Frequency 1e+7 Hz
 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
IEC 250
Dissipation Factor  0.0090
@Frequency 1e+7 Hz
0.0090
@Frequency 1e+7 Hz
 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
IEC 250
Arc Resistance 182 sec182 sec
Comparative Tracking Index 200 V200 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 3.00 µm/m-°C
@Temperature -50.0 - 200 °C
1.67 µin/in-°F
@Temperature -58.0 - 392 °F
CTE, linear, Transverse to Flow 58.0 µm/m-°C
@Temperature -50.0 - 200 °C
32.2 µin/in-°F
@Temperature -58.0 - 392 °F
Melting Point 325 °C617 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 284 °C543 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FISO 75/A
Vicat Softening Point 252 °C486 °FASTM D1525
UL RTI, Electrical 240 °C464 °F
UL RTI, Mechanical with Impact 220 °C428 °F
Flammability, UL94 V-0V-0
Oxygen Index 44 %44 %ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omya OMYACARB® 4 - LU Calcium Carbonate
Celanese Vectra® C150 Liquid Crystal Polymer (LCP), 50% Glass Reinforced
LNP Lubricomp® OCL-4036 Polyphenylene Sulfide, Carbon Fiber Reinforcement, PTFE Lubricant
RTP Company RTP 1385 TFE 15 Polyphenylene Sulfide (PPS), Carbon Fiber - PTFE Lubricated
Celanese VECTRA® 2310MT 30% Glass Filled, Medical Grade Liquid Crystal Polymer (LCP)

PHCU83 / 45823

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.