MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Renishaw 6230 Vacuum casting resin
Categories: Polymer; Thermoset

Material Notes: Description: Properties similar to ABS

Features: Good impact resistance

Suitable for: Prototype parts and low volume production

Information provided by Renishaw

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccPart A
 1.20 g/cc1.20 g/ccPart B
 1.23 g/cc1.23 g/ccCured, finished article
Viscosity 200 cP200 cPPart B
 850 cP850 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383Cured; ISO 868
Tensile Strength 67.0 MPa9720 psiCured; ISO R 527
Tensile Strength, Yield 67.0 MPa9720 psiCured; ISO R 527
Elongation at Break 14 %14 %Cured; ISO R 527
Elongation at Yield 14 %14 %Cured; ISO R 527
Tensile Modulus 1.85 GPa268 ksiCured; ISO R 527
Flexural Strength 80.0 MPa11600 psiCured; ISO 178
Flexural Modulus 1.80 GPa261 ksiCured; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²Cured; ISO 180
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C4.44 µin/in-°FCured; JIS K-6911
Thermal Conductivity 0.241 W/m-K1.67 BTU-in/hr-ft²-°FCured; ISO BS 874
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FCured, (test piece 110 mm × 12.7 mm × 6.4 mm); ISO 75
Glass Transition Temp, Tg 115 °C239 °FCured
Shrinkage 0.30 %0.30 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 35.0 - 40.0 °C95.0 - 104 °FResin Temp
Mold Temperature 70.0 °C158 °F
Pot Life  3.67 min
@Load 0.100 kg,
Temperature 35.0 °C
3.67 min
@Load 0.221 lb,
Temperature 95.0 °F
 6.00 min
@Load 0.100 kg,
Temperature 25.0 °C
6.00 min
@Load 0.221 lb,
Temperature 77.0 °F
 
Descriptive Properties
ColorMilky white
Mixing ratio by weightA:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Renishaw 420 Hand/Vacuum casting resin
Renishaw 3176 Vacuum casting resin
Renishaw 8051 Vacuum casting resin
Renishaw 8060-2 Vacuum casting resin
Renishaw 8095 Vacuum casting resin

PRENISH006 / 206369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.