MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec Sonox® P4 Piezoceramic
Categories: Ceramic; Oxide; Piezoelectric

Material Notes: Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics require very little energy and their shape potential is almost unlimited. Such properties allow this material to be used in wide-ranging apparatus and mechanical engineering applications. Sonox® P4 is designed to withstand high electrical control voltages and intense mechanical (pressure) loads. It features low dielectric loss, dielectric constants between 1000 and 1600, and high Q values (between 500 and 2000). It is well suited for high-performance ultrasonic applications in the 20 kHz to several MHz range. P4 is specifically used in ultrasonic cleaning and sonar technology.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.65 g/cc0.276 lb/in³
 
Electrical PropertiesMetricEnglishComments
Curie Temperature 325 °C617 °FTc
Dielectric Constant 660660e33 S/e0
 885885e11 S/e0
 13001300e33 t/e0
 15351535e11 t/e0
Dissipation Factor 0.00300.0030
Piezoelectric Longitudinal Coupling Factor, k33 0.680.68
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -130-130
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 455455
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 26.926.9
Piezoelectric Planar Coupling Factor, kp 0.570.57
Piezoelectric Mechanical Q 500500
Piezoelectric Shear Coupling Factor, k15 0.650.65
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 310310
Piezoelectric Transverse Coupling Factor, k31 0.310.31
 
Descriptive Properties
Aging Rates (%/decade)1.1Cf
 -3.2Ck
 -3.4Ce
Elastic Compliance (10^-12 m²/N)14.9s11^E
 18.1s33^E
Elastic Rigidity (10^10 N/m²)15.9c33^D
 4.8c55^D
Frequency Constants (kHz·mm)1340N3
 1480N1
 2000Nt
 2210Np
Piezoelectric Coupling Coefficient, kt0.5
Piezoelectric Voltage Coefficient, e33 (C/m²)15.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Sonox® P8 Piezoceramic
CeramTec Sonox® P6 Piezoceramic
CeramTec Sonox® P41 Piezoceramic
CeramTec Sonox® P5 Piezoceramic
CeramTec Sonox® P508 Piezoceramic

CCERA947 / 107547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.