MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.200 - 1.21 g/cc0.00723 - 0.0437 lb/in³Average value: 0.901 g/cc Grade Count:168
Particle Size 5.00 - 1000 µm5.00 - 1000 µmAverage value: 494 µm Grade Count:7
Viscosity 149 - 6.696e+6 cP
@Temperature 150 - 200 °C
149 - 6.696e+6 cP
@Temperature 302 - 392 °F
Average value: 864000 cP Grade Count:20
Environmental Stress Crack Resistance 100 - 1000 hour100 - 1000 hourAverage value: 423 hour Grade Count:13
Vinyl Acetate Content 2.00 - 40.0 %2.00 - 40.0 %Average value: 20.3 % Grade Count:139
Melt Flow 0.150 - 850 g/10 min0.150 - 850 g/10 minAverage value: 57.9 g/10 min Grade Count:163
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 16.0 - 98.016.0 - 98.0Average value: 80.3 Grade Count:126
Hardness, Shore D 15.0 - 67.015.0 - 67.0Average value: 35.8 Grade Count:94
Tensile Strength, Ultimate 1.60 - 26.8 MPa232 - 3890 psiAverage value: 12.6 MPa Grade Count:124
 1.40 - 51.0 MPa
@Temperature -20.0 - 49.0 °C
203 - 7400 psi
@Temperature -4.00 - 120 °F
Average value: 19.8 MPa Grade Count:11
Film Tensile Strength at Yield, MD 4.69 - 5.20 MPa680 - 754 psiAverage value: 4.86 MPa Grade Count:3
Film Tensile Strength at Yield, TD 3.90 - 4.31 MPa566 - 625 psiAverage value: 4.17 MPa Grade Count:3
Tensile Strength, Yield 2.50 - 28.3 MPa363 - 4110 psiAverage value: 7.16 MPa Grade Count:29
Film Elongation at Break, MD 320 - 800 %320 - 800 %Average value: 513 % Grade Count:6
Film Elongation at Break, TD 565 - 900 %565 - 900 %Average value: 695 % Grade Count:6
Elongation at Break 50.0 - 1300 %50.0 - 1300 %Average value: 676 % Grade Count:136
 400 - 900 %
@Temperature -20.0 - 49.0 °C
400 - 900 %
@Temperature -4.00 - 120 °F
Average value: 607 % Grade Count:11
Elongation at Yield 7.30 - 260 %7.30 - 260 %Average value: 151 % Grade Count:6
Modulus of Elasticity 0.0110 - 0.700 GPa1.60 - 102 ksiAverage value: 0.0952 GPa Grade Count:29
 0.0460 - 0.345 GPa
@Temperature -20.0 - -20.0 °C
6.67 - 50.0 ksi
@Temperature -4.00 - -4.00 °F
Average value: 0.157 GPa Grade Count:11
Flexural Modulus 0.00190 - 1.25 GPa0.276 - 181 ksiAverage value: 0.0805 GPa Grade Count:72
 0.00620 - 0.503 GPa
@Temperature -20.0 - 49.0 °C
0.899 - 73.0 ksi
@Temperature -4.00 - 120 °F
Average value: 0.128 GPa Grade Count:11
Secant Modulus 0.0210 - 1.04 GPa3.05 - 151 ksiAverage value: 0.220 GPa Grade Count:6
Tensile Impact Strength 2.50 - 945 kJ/m²1.19 - 450 ft-lb/in²Average value: 565 kJ/m² Grade Count:17
 335 - 715 kJ/m²
@Temperature -20.0 - -20.0 °C
159 - 340 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 490 kJ/m² Grade Count:11
Elmendorf Tear Strength MD 204 - 245 g204 - 245 gAverage value: 231 g Grade Count:3
Elmendorf Tear Strength TD 281 - 345 g281 - 345 gAverage value: 324 g Grade Count:3
Dart Drop Test 600 - 1400 g1.32 - 3.09 lbAverage value: 922 g Grade Count:5
Compression Set 39.0 - 100 %39.0 - 100 %Average value: 70.0 % Grade Count:11
Film Tensile Strength at Break, MD 21.0 - 41.0 MPa3050 - 5940 psiAverage value: 32.6 MPa Grade Count:7
Film Tensile Strength at Break, TD 12.0 - 32.0 MPa1740 - 4640 psiAverage value: 26.5 MPa Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10.0 - 1.00e+15 ohm-cm10.0 - 1.00e+15 ohm-cmAverage value: 6.00e+14 ohm-cm Grade Count:5
Surface Resistance 50.0 - 200 ohm50.0 - 200 ohmAverage value: 133 ohm Grade Count:3
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:3
 
Thermal PropertiesMetricEnglishComments
Melting Point 48.9 - 104 °C120 - 219 °FAverage value: 82.5 °C Grade Count:119
Vicat Softening Point 23.0 - 127 °C73.4 - 261 °FAverage value: 62.8 °C Grade Count:98
Brittleness Temperature -100 - -40.0 °C-148 - -40.0 °FAverage value: -82.6 °C Grade Count:54
Flammability, UL94 HBHBGrade Count:3
Ring & Ball Softening Point 76.0 - 220 °C169 - 428 °FAverage value: 113 °C Grade Count:47
 
Optical PropertiesMetricEnglishComments
Haze 1.30 - 5.10 %1.30 - 5.10 %Average value: 3.09 % Grade Count:8
Gloss 80.0 - 89.0 %80.0 - 89.0 %Average value: 83.2 % Grade Count:5
Transmission, Visible 80.0 %80.0 %Average value: 80.0 % Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 235 °C212 - 455 °FAverage value: 158 °C Grade Count:17
Melt Temperature 180 - 230 °C356 - 446 °FAverage value: 200 °C Grade Count:18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

O4100 / 78291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.