MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Graft Polymer GRAFTABOND™ PPH-MAH 20025 CA Maleic anhydride functioned Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: GRAFTABOND™ PPH-MAH 20025 CA is a high performance maleic anhydride functioned homo-polypropylene. The high degree of grafting adds polarity to PP matrices, which greatly improves compatibility of PP with glass reinforcements, natural and inorganic fillers. This grade is best used as coupling agent for short glass fiber reinforced PP.

Applications:

  • GRAFTABOND™ PPH-MAH 20025 CA functions as a coupling agent between reinforcing materials (glass fibers, natural and inorganic fillers) and polypropylene
  • Compatibility of polypropylene and polyamide alloys
  • Compatibility between polyolefin and polar polymers, that interact with maleic anhydride for alloying, recycling or co-extrusion purposes
  • Increased adhesion properties of polypropylene to metal surfaces.
Supplied as: Granulate.

Properties can be regulated to customer needs.

Information provided by Graft Polymer LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow  41 g/10 min
@Load 1.20 kg,
Temperature 190 °C
41 g/10 min
@Load 2.65 lb,
Temperature 374 °F
ASTM D1238
 200 g/10 min
@Load 2.16 kg,
Temperature 230 °C
200 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Descriptive Properties
Drying Loss> 0.5%, ASTM D6980 @ 105°C
Maleic Anhydride Graft Level~2.5%FTIR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graft Polymer GRAFTABOND™ PPH-MAH 15025 CA Maleic anhydride functioned Homopolymer Polypropylene
Graft Polymer GRAFTABOND™ PPH-MAH 02030 C Maleic anhydride functioned homo-polypropylene
Graft Polymer GRAFTABOND™ PPH-MAH 48025 CA Maleic anhydride functioned Homopolymer Polypropylene
Graft Polymer GRAFTABOND™ PPC-GMA 02030 C Polypropylene grafted with Glycidyl Methacrylate
Dow AMPLIFY™ GR 207 Maleic anhydride grafted (MAH) polymer

PGRAFT914 / 232345

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.