MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Sumitomo Bakelite RX® 647 Phenolic Resole Compound
Categories: Polymer; Thermoset; Phenolic; Phenolic, Resole, Glass Fiber Filled

Material Notes: RX® 647 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-5.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 g/cc1.90 g/ccASTM D792
Apparent Bulk Density 0.800 g/cc0.0289 lb/in³ASTM D1895
Water Absorption  0.040 %
@Time 86400 sec
0.040 %
@Time 24.0 hour
ASTM D570
 0.20 %
@Time 173000 sec
0.20 %
@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8585ASTM D785
Tensile Strength 72.0 MPa10400 psiASTM D638
Flexural Strength 152 MPa22000 psiASTM D790
Flexural Modulus 15.9 GPa2310 ksiASTM D790
Compressive Strength 200 MPa29000 psiASTM D695
Izod Impact, Notched 0.270 J/cm0.506 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  11.8 kV/mm
@Frequency 60 Hz
300 kV/in
@Frequency 60 Hz
SS, dry; ASTM D149
 13.8 kV/mm
@Frequency 60 Hz
351 kV/in
@Frequency 60 Hz
ST, dry; ASTM D149
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C7.78 µin/in-°FASTM E831
Thermal Conductivity 0.790 W/m-K5.48 BTU-in/hr-ft²-°FASTM C518
Deflection Temperature at 1.8 MPa (264 psi) 276 °C529 °FAs Molded; ASTM D648A
 >= 282 °C>= 540 °FPost Baked; ASTM D648A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite RX® 643 Phenolic Resole Compound
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole
Cosmic Plastics K43/6260 Mineral Filled Diallyl Iso-Phthalate Molding Compound
Cosmic Plastics K31/6220 Short Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound
Cosmic Plastics ID-50 Dacron Filled Diallyl Iso-Phthalate Molding Compound

PSUMIT763 / 194568

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.