MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GEHR Plastics PA 12 TR Transparent Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Used for optical components that benefit from the transparency and the high dynamic strength

Properties:

  • Transparency
  • Extremely high dynamic strength
  • High chemical resistance
  • High stress-cracking resistance
  • Very high toughness
  • Good weather resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccISO 1183
Moisture Absorption at Equilibrium 1.5 %1.5 %ISO 62
Water Absorption at Saturation 3.0 %3.0 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ISO 868
Ball Indentation Hardness 90.0 MPa13100 psiISO 2039
Tensile Strength at Break 45.0 MPa6530 psiISO 527
Tensile Strength, Yield 66.0 MPa9570 psiISO 527
Elongation at Break >= 50 %>= 50 %ISO 527
Elongation at Yield 6.0 %6.0 %ISO 527
Modulus of Elasticity 1.47 GPa213 ksiISO 527
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+11 ohm-cm>= 1.00e+11 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Strength 34.0 kV/mm864 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FISO 11359
Melting Point 155 °C311 °FDIN EN ISO 3146
Maximum Service Temperature, Air 100 °C212 °FUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FISO 75
Glass Transition Temp, Tg 155 °C311 °FDIN EN ISO 3146
Flammability, UL94 HBHBUL 94
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"transparent" but not quantified
 
Compliance PropertiesMetricEnglishComments
FDA YesYesPhysiological indifference; NSF-61, FDA, data taken from raw material
 
Descriptive Properties
Bondabilityyes
Colortransparent
Physiological indifferenceyes, EEC
UV Stabilizationyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Trogamid® CX9701 Transparent Nylon
Evonik VESTAMID® LX9008 PA 12
Evonik Trogamid® CX7323 Transparent Nylon
Evonik VESTAMID® EX9200 PA 12
Alcoa KAMA 7210 Clear Random Copolymer Polypropylene (PP)

PGEHR017_a / 150419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.