MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SK Chemicals Saran® 520 Clear Plastic Barrier Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyvinyl Dichloride (PVDC)

Material Notes: Saran™ 520 is a clear biaxially oriented monolayer barrier film, designed for unit packaging and other applications. It is available in 2 gauge.

SK Global Chemical has purchased the SARAN® resin business from Dow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 1.94 g/m²/day
@Temperature 37.8 °C
0.125 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM F1249-90
Oxygen Transmission 0.571 cc-mm/m²-24hr-atm1.45 cc-mil/100 in²-24hr-atm10% RH; ASTM D3985
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 95 %95 %ASTM D882
Film Elongation at Break, TD 80 %80 %ASTM D882
Secant Modulus, MD 0.6895 GPa100.0 ksi2% Secant; ASTM D882
Secant Modulus, TD 0.6136 GPa89.00 ksi2% Secant; ASTM D882
Coefficient of Friction, Dynamic 0.300.30Film to Metal; ASTM D1894
Film Tensile Strength at Break, MD 110 MPa16000 psiASTM D882
Film Tensile Strength at Break, TD 131 MPa19000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 8.0 %
@Temperature 100 °C
8.0 %
@Temperature 212 °F
10 min at 100°C Air, unrestrained; ASTM D1204
Shrinkage, TD 4.0 %
@Temperature 100 °C
4.0 %
@Temperature 212 °F
10 min at 100°C Air, unrestrained; ASTM D1204
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %3.0 %ASTM D1003
Gloss 105 %105 %45°; ASTM D2457
Transmission, Visible 73 %73 %Clarity; ASTM D1746
 
Descriptive Properties
Yield in2/lb8100Calculated

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SK Chemicals Saran® 540 Clear Plastic Barrier Film
SK Chemicals Saran® 28 Clear Plastic Barrier Film
SK Chemicals Saran® 18L Clear Plastic Barrier Film
SK Chemicals Saran® 520 Vapor Retarder Tape
SK Chemicals Saran® 560 Clear Plastic Barrier Film

PDOW1414 / 30632

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.