MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ferrite 5, Sintered Iron-Strontium Oxide Hard Magnetic Material
Categories: Ceramic; Oxide

Material Notes: SrO-6Fe2O3

Key Words: SrO-6Fe2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.50 g/cc0.163 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cm
Magnetic Coercive Force, Hc 3142 Oe3142 Oe
Magnetic Remanence, Br 3550 Gauss3550 Gauss
Magnetic Maximum Energy Product, BH 3.02 MGOe3.02 MGOe
Curie Temperature 460 °C860 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 400 °C752 °F
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 6.0 %6.0 %
 
Descriptive Properties
Demagnetization Induction, Bd (Tesla)0.173
Intrinsic Magnetic Coercive Force, HCi (Oe)3607

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ferrite A, Bonded Iron-Barium Oxide Hard Magnetic Material
Ferrite 4, Sintered Iron-Strontium Oxide Hard Magnetic Material
HGC-1 Precious dental alloy
Ferrite 3, Sintered Iron-Barium Oxide Hard Magnetic Material
Gold (I) Sulfide, Au2S

BFERR04 / 100426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.