MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borpact™ BC914TF Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Borpact™ BC914TF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. This grade is especially developed for the manufacturing of unoriented film for various film processing technologies like cast film process, conventional blown film process with air cooling and roll stack process for thermoformable films/sheets. Optical properties will not be deteriorated as with conventional homo or copolymers at these temperatures. Applications: Borpact™ BC914TF is recommended for label film, lamination films, food packaging, map trays, stand up pouch film, vegetable trays, and inner layer in coextrusion.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 1.45 GPa210 ksi50% humidity; ISO 178
Charpy Impact, Notched  0.200 J/cm²
@Temperature -20.0 °C
0.952 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °F
Vicat Softening Point 154 °C
@Load 1.02 kg
309 °F
@Load 2.25 lb
A50; ISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BC612WG Polypropylene Copolymer
Borealis BC650MO Polypropylene Copolymer
Borealis BC142MO Polypropylene Copolymer
Borealis BC918CF Polypropylene Copolymer
Borealis BC545MO Polypropylene Copolymer

PBOREA380 / 108639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.