MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ecomass® Ecomass® 5033ZG87 SS/Tungsten Powder filled Styrene Isoprene Styrene (SIS)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Nontoxic alternative to Lead (Pb), weighting and balancing applications. High specific gravity, SS/Tungsten Powder filled Styrene Isoprene Styrene (SIS), flexible. Injection molding, pellet form.

Information provided by Ecomass Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 4.50 g/cc4.50 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 13.1 MPa1900 psiASTM D638
Elongation at Break 16 %16 %ASTM D638
Tensile Modulus 0.683 GPa99.0 ksiASTM D638
Flexural Strength 24.1 MPa3500 psiASTM D790
Flexural Modulus 0.793 GPa115 ksiASTM D790
Izod Impact, Notched 3.74 J/cm7.00 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.20 ohm0.20 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 - 191 °C220 - 375 °F
 
Processing PropertiesMetricEnglishComments
Mold Temperature 21.1 - 43.3 °C70.0 - 110 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ecomass® Ecomass® 4150TU96 Tungsten Powder filled Polyphenylene Sulfide (PPS)
Ecomass® 720ZD88 Tungsten Filled ABS
Ecomass® 4703ZD95 Tungsten Filled Polyurethane
Ecomass® 3608TU96 Tungsten Filled Polyethylene
Ecomass® 1080ZD96 Tungsten Filled Polyamide

PECOM936 / 209806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.