MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxy Technology EPO-TEK® H20-FC Electrically Conductive Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Product Description: EPO-TEK®H20E-FC is a two-component, electrically conductive, snap curing epoxy for photovoltaic thin film module stringing, semiconductor packaging and PCB circuit assembly.

Advantages & Application Notes:

  • It is a snap cure version of EPO-TEK® H20E, designed for snap cure at 140°C and <15 minute cure at 120°C.
  • Strengths include dispensable rheology and a long pot life.
  • Suggested Applications:
    • Semiconductor: die-attaching IC’s onto Cu plated lead-frame yielding semiconductor plastic package formats.
    • PCB: solder replacement adhesive, electrical bridge of Au, Ag and AgPd electrode pads onto Au- or Cu-plated PCBs.
    • Photovoltaics:
      • Electrically conductive stringing of thin film, organic and crystalline Si solar cells.
      • Compatible with SnCu and AgCu metalized solar ribbons, and TCO substrates such as ITO, ZnO and SnO.
      • Versatility in ribbon bonding geometries, such as dotted or continuous line.
      • In-line/in-situ curing processes in <1 minute at 140°C can be achieved.
      • Reliable green strength holds solar ribbons in position prior to cure.
      • Low temperature cure is well suited for CIGS and OPV/DSC solar cells requiring a low temperature process.
      • Suitable for use on IEC 61646, IEC 61730 and UL 1703 certified solar panels.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.51 g/cc2.51 g/ccPart B
 3.80 g/cc3.80 g/ccPart A
Particle Size <= 45 µm<= 45 µm
Viscosity 2361 cP
@Temperature 23.0 °C
2361 cP
@Temperature 73.4 °F
50 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555
Tensile Modulus 6.39 GPa928 ksiStorage
Shear Strength >= 13.8 MPa>= 2000 psiLap
 >= 23.4 MPa>= 3400 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00040 ohm-cm<= 0.00040 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 56.0 µm/m-°C31.1 µin/in-°FBelow Tg
 233 µm/m-°C129 µin/in-°FAbove Tg
Thermal Conductivity 2.63 W/m-K18.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg 85.0 °C185 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 392 °C738 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 120 °C
0.250 hour
@Temperature 248 °F
Minimum Bond Line
 35.0 min
@Temperature 140 °C
0.583 hour
@Temperature 284 °F
Minimum Bond Line
 45.0 min
@Temperature 80.0 °C
0.750 hour
@Temperature 176 °F
Minimum Bond Line
Pot Life 1200 min1200 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorSilverPart A
 SilverPart B
ConsistencySmooth thixotropic paste
Mix Ratio by Weight1:1
Number of ComponentsTwo
Thixotropic Index4.62
Weight Loss0.73%200°C
 1.67%250°C
 2.37%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® E3001 Electrically Conductive, Silver Epoxy
Bismuth Telluride, Bi2Te3 (Tellurobismuthite)
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® E3001-6 Electrically Conductive, Silver Epoxy

PPOXYT030 / 141069

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.