MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Alpha/Beta Titanium Alloy
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Alpha/Beta Titanium Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.25 - 4.84 g/cc0.154 - 0.175 lb/in³Average value: 4.53 g/cc Grade Count:84
Porosity 2.00 - 4.00 %2.00 - 4.00 %Average value: 2.83 % Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 290 - 411290 - 411Average value: 348 Grade Count:23
Hardness, Knoop 315 - 450315 - 450Average value: 379 Grade Count:23
Hardness, Rockwell C 30.0 - 44.030.0 - 44.0Average value: 36.9 Grade Count:28
Hardness, Vickers 304 - 480304 - 480Average value: 364 Grade Count:26
Tensile Strength, Ultimate 200 - 1580 MPa29000 - 229000 psiAverage value: 1030 MPa Grade Count:86
Tensile Strength, Yield 680 - 1410 MPa98600 - 205000 psiAverage value: 963 MPa Grade Count:86
Elongation at Break 3.00 - 20.0 %3.00 - 20.0 %Average value: 11.2 % Grade Count:83
Reduction of Area 10.0 - 50.0 %10.0 - 50.0 %Average value: 26.5 % Grade Count:52
Modulus of Elasticity 100 - 126 GPa14500 - 18300 ksiAverage value: 114 GPa Grade Count:71
Compressive Yield Strength 860 - 1280 MPa125000 - 186000 psiAverage value: 1030 MPa Grade Count:10
Notched Tensile Strength 690 - 1550 MPa100000 - 225000 psiAverage value: 1350 MPa Grade Count:11
Ultimate Bearing Strength 1740 - 2300 MPa252000 - 334000 psiAverage value: 2090 MPa Grade Count:7
Bearing Yield Strength 1350 - 1900 MPa196000 - 276000 psiAverage value: 1630 MPa Grade Count:7
Poissons Ratio 0.310 - 0.3420.310 - 0.342Average value: 0.322 Grade Count:47
Fatigue Strength 140 - 1160 MPa20300 - 168000 psiAverage value: 517 MPa Grade Count:37
Fracture Toughness 24.0 - 105 MPa-m½21.8 - 95.6 ksi-in½Average value: 56.6 MPa-m½ Grade Count:18
Shear Modulus 41.0 - 48.3 GPa5950 - 7010 ksiAverage value: 43.7 GPa Grade Count:49
Shear Strength 550 - 950 MPa79800 - 138000 psiAverage value: 711 MPa Grade Count:7
Charpy Impact 9.50 - 25.0 J7.01 - 18.4 ft-lbAverage value: 18.9 J Grade Count:15
Bend Radius, Minimum 3.00 - 5.00 t3.00 - 5.00 tAverage value: 4.81 t Grade Count:13
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000920 - 0.000205 ohm-cm0.0000920 - 0.000205 ohm-cmAverage value: 0.000173 ohm-cm Grade Count:60
Magnetic Permeability 1.00 - 1.001.00 - 1.00Average value: 1.00 Grade Count:28
Magnetic Susceptibility 0.00000330 - 0.000003510.00000330 - 0.00000351Average value: 0.00000333 Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.71 - 11.7 µm/m-°C4.28 - 6.50 µin/in-°FAverage value: 9.23 µm/m-°C Grade Count:61
Specific Heat Capacity 0.368 - 0.670 J/g-°C0.0880 - 0.160 BTU/lb-°FAverage value: 0.538 J/g-°C Grade Count:57
Thermal Conductivity 6.10 - 10.9 W/m-K42.3 - 75.6 BTU-in/hr-ft²-°FAverage value: 7.13 W/m-K Grade Count:60
Melting Point 1570 - 1700 °C2850 - 3090 °FAverage value: 1640 °C Grade Count:51
Solidus 1300 - 1630 °C2370 - 2960 °FAverage value: 1590 °C Grade Count:24
Liquidus 1640 - 1700 °C2980 - 3090 °FAverage value: 1660 °C Grade Count:50
Maximum Service Temperature, Air 315 - 480 °C599 - 896 °FAverage value: 372 °C Grade Count:31
Beta Transus 785 - 1050 °C1450 - 1920 °FAverage value: 965 °C Grade Count:66
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.00 - 7.30 %2.00 - 7.30 %Average value: 5.73 % Grade Count:87
Carbon, C 0.0100 - 0.800 %0.0100 - 0.800 %Average value: 0.0783 % Grade Count:71
Chromium, Cr 1.50 - 4.00 %1.50 - 4.00 %Average value: 2.83 % Grade Count:9
Copper, Cu 0.0500 - 1.00 %0.0500 - 1.00 %Average value: 0.511 % Grade Count:7
Hydrogen, H 0.00500 - 0.125 %0.00500 - 0.125 %Average value: 0.0303 % Grade Count:67
Iron, Fe 0.100 - 3.00 %0.100 - 3.00 %Average value: 0.335 % Grade Count:79
Manganese, Mn 0.0500 - 8.00 %0.0500 - 8.00 %Average value: 2.72 % Grade Count:3
Molybdenum, Mo 0.500 - 6.50 %0.500 - 6.50 %Average value: 4.28 % Grade Count:39
Niobium, Nb (Columbium, Cb) 6.50 - 7.50 %6.50 - 7.50 %Average value: 7.00 % Grade Count:3
Nitrogen, N 0.0120 - 0.0700 %0.0120 - 0.0700 %Average value: 0.0398 % Grade Count:73
O + 2N 0.270 %0.270 %Average value: 0.270 % Grade Count:3
Oxygen, O 0.0800 - 0.250 %0.0800 - 0.250 %Average value: 0.167 % Grade Count:75
Silicon, Si 0.100 - 0.700 %0.100 - 0.700 %Average value: 0.354 % Grade Count:13
Tantalum, Ta 0.500 %0.500 %Average value: 0.500 % Grade Count:3
Tin, Sn 1.50 - 11.5 %1.50 - 11.5 %Average value: 2.74 % Grade Count:39
Titanium, Ti 77.9 - 92.5 %77.9 - 92.5 %Average value: 86.8 % Grade Count:88
Vanadium, V 1.00 - 6.00 %1.00 - 6.00 %Average value: 4.15 % Grade Count:46
Zirconium, Zr 1.50 - 6.00 %1.50 - 6.00 %Average value: 3.36 % Grade Count:28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Beta Titanium Alloy
Overview of materials for Alpha/Near Alpha Titanium Alloy
Titanium, Ti
Overview of materials for Nickel Alloy
Titanium Alloys, General

M01070 / 81698

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.