MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vyncolit BXE7665 Glass Filled Phenolic Molding Compound
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.

Information provided by Sumitomo Bakelite North America, Inc.

Key Words: PF-(GF+MD)65
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.630 g/cc0.0228 lb/in³ISO 60
Density 1.90 g/cc0.0686 lb/in³ISO 1183
Water Absorption 0.040 %0.040 %ISO 62
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 101 MPa14600 psiISO 527-1
Elongation at Break 0.56 %0.56 %ISO 527-1
Tensile Modulus 22.0 GPa3190 ksiISO 527-1
Flexural Strength 205 MPa29700 psiISO 178
Flexural Modulus 21.0 GPa3050 ksiISO 178
Compressive Strength 293 MPa42500 psiISO 604
Charpy Impact Unnotched 1.17 J/cm²5.57 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.10e+14 ohm-cm8.10e+14 ohm-cmIEC 60093
Surface Resistance 4.30e+13 ohm4.30e+13 ohmIEC 60093
Dielectric Strength 19.0 kV/mm483 kV/inIEC 60243-1
Comparative Tracking Index 200 V200 VIEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C7.78 µin/in-°FTMA
CTE, linear, Transverse to Flow 31.0 µm/m-°C17.2 µin/in-°FTMA
Thermal Conductivity 0.480 W/m-K3.33 BTU-in/hr-ft²-°FASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) >= 195 °C>= 383 °FISO 75 Af
Deflection Temperature at 8.0 MPa 168 °C334 °FISO 75 Cf
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage 0.040 %0.040 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
Molding MethodCompression
 Injection
 Transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic

PVYNC946 / 142721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.