MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Pro-fax™ SD183 Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Description: Pro-fax™ SD183 medium impact polypropylene copolymer resin is extremely resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of properties and is suited for injection molding or extrusion applications. Pro-fax™ SD183 resin has a UL yellow card RTI of 65°C and a flame rating of UL94HB; these apply to all colors at a minimum thickness of 0.043 inches. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Appliances

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.6 MPa4000 psiASTM D 638
Elongation at Yield 10 %10 %ASTM D 638
Flexural Modulus, 1% Secant 1170 MPa170000 psi0.05 in/min; ASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/in73°F; ASTM D256
Gardner Impact 27.1 J
@Temperature -30.0 °C
20.0 ft-lb
@Temperature -22.0 °F
ASTM D3029, tested in accordance with ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C189 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax 7624 Polypropylene Impact Copolymer, Heat- and Extraction-Resistant
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer
LyondellBasell Pro-fax™ SR257M Polypropylene Copolymer
LyondellBasell Pro-fax™ SC973 Polypropylene Copolymer
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer

PMO883 / 53872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.