MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-BOND® 1075 Silicone RTV Adhesive/Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposure to atmospheric moisture, and contains no acetic acid or other corrosive agents

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 - 2.25 g/cc1.75 - 2.25 g/cc
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Thickness >= 254 microns>= 10.0 milRecommended
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 0.689 MPa>= 100 psiLap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.010 ohm-cm0.010 ohm-cmDC
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 23.0 °C
168 hour
@Temperature 73.4 °F
Working Life 15.0 min15.0 min
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
BinderSilicone
ConsistencyMedium paste
Coverage17 cm2 / g
FillerAg/Al
Mix Ratio1-part

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Chemical Concepts Chem-Set™ RTV 6500 Silicone (Red)
Dow 1437 INDUSTRIAL SEALANT AND ADHESIVE
Momentive Performance Materials TSE392 One Component RTV Adhesive Sealant/Coating, Clear/White
CHT Group QM 262 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material

PCHOME036 / 28258

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.