MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Norton® PVDF Fluoropolymer Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Features/Benefits:
  • Excellent weatherability
  • High dielectric strength
  • Excellent chemical and abrasion resistance
  • Thermoformable
  • Product available in widths up to 60"
  • Product available with thicknesses from 0.001" (0.0254 mm) to 0.020" (0.5 mm)
  • Temperature range of -62°C (-80°F) to 150°C (300°F)
Weatherable, Chemically Resistant Fluoropolymer Film
Norton® PVDF film is manufactured from polyvinylidene fluoride resin. This product offers the best weathering characteristics of any fluoropolymer film available. Norton® PVDF provides very good performance when subjected to severe conditions such as heat fluctuation, UV exposure, and corrosive environments. Norton® PVDF is manufactured to strict standards for gels and gauge control, offering the best value for fluoropolymer performance of any film. This material also performas over a wide temperature range, from -62°C (-80°F) to 150°C (300°F).

Chemical Protection
Norton® PVDF film protects against exposure to many common acids, oxidizing agents, and organics. This broad range of chemical resistance makes Norton® PVDF an excellent candidate for pump diaphragms and tank linings. The thin gauge films offer bondability for protection of equipment exposed to air pollutants, corrosive media, and weather.

Decorative Applications
Norton® PVDF film can be adaptable to metallizing or printing for a variety of protective applications. The excellent chemical resistance to a wide tange of cleaners and harsh cleaning agents used in high traffic applications offers long maintenance performance. Norton® PVDF carries a UL V-0 flammability rating, which signifies self-extinguishing performance suited for aircraft interior panel applications.

Weathering Applications
The outstanding weatherability of Norton® PVDF film makes it an excellent candidate for products with outdoor exposures. Vinyl siding is protected with excellent chemical and abrasion resistance of Norton® PVDF film. The fluoropolymer properties are impervious to UV expsure and eliminate wear due to water and chemical exposures. PVDF = polyvinylidene fluoride
Used for Chemical Process, Electrical/Electronics, Protective/Decorative.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/ccASTM D-792
Water Absorption <= 0.040 %<= 0.040 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.5 - 49.6 MPa5000 - 7200 psiASTM D-882
Elongation at Break 100 - 250 %100 - 250 %ASTM D-882
Tensile Modulus 2.48 GPa360 ksiASTM D-882
Flex Crack Resistance 2600026000Cycles Fold Endurance (MIN); ASTM D2176
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmASTM D-257
Dielectric Constant 8.2 - 10
@Frequency 1000 Hz
8.2 - 10
@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 157 kV/mm4000 kV/inASTM D-149
Dissipation Factor 0.0050 - 0.0200.0050 - 0.020ASTM D-150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 119 - 139 µm/m-°C
@Temperature 20.0 °C
66.0 - 77.0 µin/in-°F
@Temperature 68.0 °F
ASTM D-696
Specific Heat Capacity 1.17 - 1.59 J/g-°C0.280 - 0.380 BTU/lb-°F
Thermal Conductivity 0.199 W/m-K1.38 BTU-in/hr-ft²-°FASTM D-2863
Melting Point 174 °C345 °FASTM D-3418
Maximum Service Temperature, Air 129 °C265 °FUL-746 B
Flammability, UL94 V-0V-0
Oxygen Index >= 44 %>= 44 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.401.40ASTM D542

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Norton® PFA Fluoropolymer Film
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.003" thick)
Saint-Gobain Norton® FEP Fluoropolymer Film
Overview of materials for Polyester Film

PSTGQZ163 / 68677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.