MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® CA116-201 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN CA116-201 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-201 is part of the HUNTSMAN film and sheet product range and offers a specially designed, flexible plasticizer free product suitable for the preparation of extruded films.

Performance Features:

  • Low melt temperature
  • High crystallization rate
  • Good low temperature flexibility
  • Good processability
Applications:
  • Adhesive film
  • Lamination

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D792
Melt Index of Compound 15 g/10 min
@Load 5.00 kg,
Temperature 190 °C
15 g/10 min
@Load 11.0 lb,
Temperature 374 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595Injection molded parts; ASTM D2240
Tensile Strength at Break 33.0 MPa4790 psiInjection molded parts; DIN 53504
Elongation at Break 400 %400 %Injection molded parts; DIN 53504
100% Modulus 6.07 MPa
@Strain 100 %
880 psi
@Strain 100 %
Injection molded parts; ASTM D412
300% Modulus 6.58 MPa
@Strain 300 %
954 psi
@Strain 300 %
Injection molded parts; ASTM D412
Tear Strength 92.9 kN/m530 pliInjection molded parts; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Melting Point 90.0 - 120 °C194 - 248 °FTMA Melt Range
 
Processing PropertiesMetricEnglishComments
Feed Temperature 160 °C320 °FExtrusion
Middle Barrel Temperature 170 °C338 °FExtrusion
Adapter Temperature 170 °C338 °FExtrusion
Die Temperature 170 °C338 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® CA116-205 TPU-Polyester
Huntsman IROGRAN® CA 117-200 DP TPU-Polyester
Huntsman IROGRAN® PS 456-202 TPU-Polyester
Huntsman IROGRAN® CA116-203 TPU-Polyester
Huntsman IROGRAN® A 85 P 4394 FCM Ether-Based TPU-For Food Contact

PHUQ106 / 159479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.