MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Main Charactistics: Stress resistant; High impact strength at 196 ° C
Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine Tools

Information provided by Zedex

Key Words: PEEK
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Water Absorption 0.050 %
@Temperature 23.0 °C
0.050 %
@Temperature 73.4 °F
RMC 93%; DIN EN ISO 62
Moisture Absorption at Equilibrium 0.10 %0.10 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 100>= 100DIN 53505
Hardness, Shore D 8585DIN 53505
Ball Indentation Hardness 190 MPa27600 psiDIN 2039
Tensile Strength at Break 98.0 MPa14200 psiDIN EN ISO 527
Tensile Strength 113 MPa16400 psiDIN EN ISO 527
Tensile Strength, Yield 78.0 MPa11300 psiElastic Limit
 113 MPa16400 psiDIN EN ISO 527
Tensile Stress at Strain 29.0 MPa
@Strain 1 %,
Time 3.60e+6 sec
4210 psi
@Strain 1 %,
Time 1000 hour
DIN 53444
Elongation at Break 9.0 %9.0 %
 9.0 %9.0 %DIN EN ISO 527
Elongation at Yield 1.3 %1.3 %Elastic Yield Point
 5.0 %5.0 %DIN EN ISO 527
 5.0 %5.0 %Elongation at Maximum Force; DIN EN ISO 527
Tensile Modulus 4.40 GPa638 ksiDIN EN ISO 527
Flexural Strength 119 MPa17300 psiOuter Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
 159 MPa23100 psiDIN EN ISO 178
Flexural Modulus 2.937 GPa426.0 ksiDIN EN ISO 178
Flexural Strain at Yield 6.6 %6.6 %DIN EN ISO 178
Compressive Strain at Yield 12.5 %12.5 %Nominal; DIN EN ISO 604
Compressive Yield Strength 122 MPa17700 psiElastic Limit
 146 MPa21200 psiDIN EN ISO 604
Compressive Strength  40.0 MPa
@Time 3.60e+7 sec
5800 psi
@Time 10000 hour
 103 MPa
@Time 360000 sec
14900 psi
@Time 100 hour
 130 MPa
@Time 36.0 sec
18900 psi
@Time 0.0100 hour
 36.0 MPa
@Strain 3.5 %
5220 psi
@Strain 3.5 %
DIN EN ISO 604
Compressive Modulus 2.85 GPa413 ksiDIN EN ISO 604
Fatigue Strength 65.0 MPa
@# of Cycles 1.00e+6
9430 psi
@# of Cycles 1.00e+6
1 Hz
K Factor (ISO)  1.2 µm/km
@Temperature 200 °C
1.2 µm/km
@Temperature 392 °F
 3.7 µm/km
@Temperature 240 °C
3.7 µm/km
@Temperature 464 °F
 9.1 µm/km
@Temperature 100 °C
9.1 µm/km
@Temperature 212 °F
 12 µm/km
@Temperature 20.0 °C
12 µm/km
@Temperature 68.0 °F
Charpy Impact Unnotched NBNBEN ISO 179/1eU
Charpy Impact, Notched 0.620 J/cm²2.95 ft-lb/in²EN ISO 179/1eA
Coefficient of Friction, Dynamic  0.14
@Temperature 20.0 °C
0.14
@Temperature 68.0 °F
Dry Operation
 0.21
@Temperature 100 °C
0.21
@Temperature 212 °F
Dry Operation
Coefficient of Friction, Static 0.18
@Temperature 20.0 °C
0.18
@Temperature 68.0 °F
Dry Operation
Tensile Creep Modulus, 1000 hours 2780 MPa403000 psiAt 1% Deformation; DIN 53444
Limiting Pressure Velocity 0.300 MPa-m/sec8570 psi-ft/minv = 200m/min
 0.33333 MPa-m/sec9516.6 psi-ft/minv = 100m/min
 0.91666 MPa-m/sec26171 psi-ft/minv = 10m/min
 1.00 MPa-m/sec28600 psi-ft/minv = 1m/min
Compression Set 8.3 %8.3 %Elastic Compression Limit
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+15 ohm-cm4.00e+15 ohm-cmIEC 93
Surface Resistance 7.80e+11 ohm7.80e+11 ohmIEC 93
Dielectric Constant 3.0
@Frequency 110 Hz
3.0
@Frequency 110 Hz
IEC 250
Dielectric Strength 26.0 kV/mm660 kV/inIEC 243
Dissipation Factor 0.00200.0020IEC 112
 0.053
@Frequency 110 Hz
0.053
@Frequency 110 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  58.0 µm/m-°C
@Temperature <=100 °C
32.2 µin/in-°F
@Temperature <=212 °F
ISO E 830
 58.0 µm/m-°C
@Temperature <=150 °C
32.2 µin/in-°F
@Temperature <=302 °F
ISO E 831
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°FDSC
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FDIN 52612
Melting Point 340 °C644 °FDSC
Maximum Service Temperature, Air 140 °C284 °FPressed Bushings
 250 °C482 °FContinuous
 260 °C500 °FShort Term (3h)
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °FDIN EN ISO 75
Glass Transition Temp, Tg 146 °C295 °FDSC
Flammability, UL94 V-0V-0
 
Descriptive Properties
Alignment Adjustment4Nominal Scale: 1, low; 10, high
Chemical Sterilization10Nominal Scale: 1, low; 10, high
ColorBlack
Creep Resistance5Nominal Scale: 1, low; 10, high
Dimensional Stability with Thermal Expansion5Nominal Scale: 1, low; 10, high
Free from SiliconApplicable
Gamma-rays Radiation Sterilization10Nominal Scale: 1, low; 10, high
High Precision Bushings (negative clearance)Applicable
Injection Molded PartsApplicable
Machined PartsApplicable
Moist Heat Sterilization10Nominal Scale: 1, low; 10, high
Plastic GranulesApplicable
Resistance Against dust, Dirt, Abrasive Substances7Nominal Scale: 1, low; 10, high
Resistance Against Hot Water200
Resistance to Chemicals8Nominal Scale: 1, low; 10, high
Resistant Against DisinfectantApplicable
Rods up to Øe (de)Applicable
ROHS/WEEEApplicable
Sheets up to Maximum ThicknessApplicable
Sliding Velocity100
Suitable for Outdoor Use7Nominal Scale: 1, low; 10, high
Suitable for Use in WaterApplicable
Suitable for VacuumApplicable
Tubes (hollow rods) up to Øe (de)Applicable
UV Rays Resistance9Nominal Scale: 1, low; 10, high
UV-Sterilization7Nominal Scale: 1, low; 10, high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Silicon Nitride/Aluminum Nitride/Aluminum Oxide (Sialon)
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Asahi Kasei Leona™ 53G33 Polyamide 66, Heat Stabilized, GF Reinforced
Asahi Kasei Leona® 1300S Nylon 66
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets

PZEDEX08 / 122123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.