MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the efficiency of this strengthening dispersion, Ferrium® C64™ achieves carburized surface hardness superior to current gear steels with the added benefit of increased core properties. C64™ should be considered for use in applications that require high case hardness, high strength, high toughness, and thermal resistance. C64™ has very high hardenability and only requires mild quenching.

Typical Applications: Power transmission shafts, gears and other demanding applications in aerospace, energy, and racing/off-road/mission-critical vehicles and other industries where weight savings, compactness, high temperature resistance and high surface fatigue resistance are valued.

Workability:
Fording: Forge at 1800-2100°F (982-1149°C)

Heat Treatment:
Normalizing: Heat uniformly to 1875°F(1024°C) and air cool..
Annealing: Heat uniformly to 1250°F(677°C), hold for 2 to 8 hours and air cool.. Hardness should be less than 327 HBW.
Carburizing and Hardening: Vacuum carburize at 1830°F (1000°C), followed by quenching in gas (1.5 Bar Nitrogen or higher) or oil medium.
Refrigerate: To obtain optimum case hardness, a refrigeration treatment at -100°F (-73°C) or lower for 1 hour is recommended. This should be performed with minimal delay after completion of the quench.
Temper: At 925°F (496°C)

Product Forms: Ferrium® C64™ is manufactured in typical ingot, bar and billet forms.

Ferrium is designed by Questek Innovations, LLC. and is manufactured by Latrobe Specialty Steel under license.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.98 g/cc0.288 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 42.542.5Distance from Quenched End 1 3/4 [in]
 42.542.5Distance from Quenched End 2 [in]
 4343Distance from Quenched End 1/4 [in]
 4343Distance from Quenched End 1/2 [in]
 4343Distance from Quenched End 3/4 [in]
 4343Distance from Quenched End 1 [in]
 4343Distance from Quenched End 1 1/4 [in]
 4343Distance from Quenched End 1 1/2 [in]
 48 - 5048 - 50Typical Core Hardness
 62 - 6462 - 64Typical Case Hardness
Tensile Strength, Ultimate 1580 MPa229000 psi
Tensile Strength, Yield 1370 MPa
@Strain 0.2 %
199000 psi
@Strain 0.2 %
Elongation at Break 18 %18 %
Reduction of Area 75 %75 %
Fatigue Strength  1520 MPa
@# of Cycles 330000
220000 psi
@# of Cycles 330000
 1520 MPa
@# of Cycles 550000
220000 psi
@# of Cycles 550000
 1520 MPa
@# of Cycles 1.20e+6
220000 psi
@# of Cycles 1.20e+6
 1590 MPa
@# of Cycles 130000
230000 psi
@# of Cycles 130000
 1590 MPa
@# of Cycles 250000
230000 psi
@# of Cycles 250000
 1590 MPa
@# of Cycles 2.50e+6
230000 psi
@# of Cycles 2.50e+6
 1650 MPa
@# of Cycles 53000
240000 psi
@# of Cycles 53000
 1650 MPa
@# of Cycles 110000
240000 psi
@# of Cycles 110000
 1650 MPa
@# of Cycles 190000
240000 psi
@# of Cycles 190000
 1690 MPa
@# of Cycles 70000
245000 psi
@# of Cycles 70000
 1690 MPa
@# of Cycles 110000
245000 psi
@# of Cycles 110000
 1690 MPa
@# of Cycles 210000
245000 psi
@# of Cycles 210000
 1780 MPa
@# of Cycles 100000
258000 psi
@# of Cycles 100000
 1780 MPa
@# of Cycles 190000
258000 psi
@# of Cycles 190000
 1830 MPa
@# of Cycles 49000
265000 psi
@# of Cycles 49000
 1830 MPa
@# of Cycles 80000
265000 psi
@# of Cycles 80000
 1830 MPa
@# of Cycles 100000
265000 psi
@# of Cycles 100000
Fracture Toughness 93.4 MPa-m½85.0 ksi-in½
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.32 µm/m-°C
@Temperature 24.0 - 204 °C
5.18 µin/in-°F
@Temperature 75.2 - 399 °F
 9.53 µm/m-°C
@Temperature 24.0 - 93.0 °C
5.29 µin/in-°F
@Temperature 75.2 - 199 °F
 9.57 µm/m-°C
@Temperature 24.0 - 316 °C
5.32 µin/in-°F
@Temperature 75.2 - 601 °F
 9.95 µm/m-°C
@Temperature 24.0 - 427 °C
5.53 µin/in-°F
@Temperature 75.2 - 801 °F
 10.25 µm/m-°C
@Temperature 24.0 - 538 °C
5.694 µin/in-°F
@Temperature 75.2 - 1000 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.11 %0.11 %
Chromium, Cr 3.5 %3.5 %
Cobalt, Co 16.3 %16.3 %
Iron, Fe 70.62 %70.62 %
Molybdenum, Mo 1.75 %1.75 %
Nickel, Ni 7.5 %7.5 %
Tungsten, W 0.20 %0.20 %
Vanadium, V 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 9310 VAC-ARC Premium Carburizing Steel
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties
ATI Allvac® 9310 UNS G93106, UNS H93100 Specialty Steel

NQUEST003 / 121071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.