MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® TX sheet Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Extended weatherability transportation glazing Makrolon® TX sheet is a hard-coated polycarbonate product designed to meet demanding transportation glazing applications. The sheet provides high impact performance at half the weight of the glass. The advanced hard coat technology provides extended outdoor weathering properties and significantly enhances abrasion and chemical resistance. Makrolon TX meets DOT/ ANSI Z26.1 Item AS-4 and is available in clear, as well as a variety of standard and custom tints.

Applications: Truck cabs, automotive roofs, and other transportation glazing

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 65.5 MPa9500 psiASTM D638
Tensile Modulus 2.34 GPa339 ksiASTM D638
Flexural Strength 93.1 MPa13500 psiASTM D790
Izod Impact, Notched 8.54 J/cm
@Thickness 3.17 mm
16.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D256
Impact Test >= 63.7 J
@Thickness 3.17 mm
>= 47.0 ft-lb
@Thickness 0.125 in
ASTM D3763
Taber Abrasion, mg/1000 Cycles 2.0
@Load 0.500 kg
2.0
@Load 1.10 lb
CS-10F Wheel; ASTM D1044
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.5 µm/m-°C37.5 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Yellow Index 0.50 %0.50 %
 2.0 %2.0 %8 years
 3.5 %3.5 %16 years
Transmission, Visible 84 %
@Thickness 5.99 mm
84 %
@Thickness 0.236 in
ASTM D1003
 
Descriptive Properties
Chemical ResistanceAcetone>24 Hrs
 Ammonia (10% concentration)>24 Hrs
 Antifreeze (50/50)>24 Hrs
 Benzene>24 Hrs
 Bleach (Clorox concentrated)>24 Hrs
 Chloroform>24 Hrs
 Denatured Alcohol>24 Hrs
 Di (2-ethylhexyl) phthalate>24 Hrs
 Diesel Oil>24 Hrs
 Hydrochloric Acid (20%)>24 Hrs
 Isopropyl Alcohol (IPA)>24 Hrs
 Kerosene>24 Hrs
 Methyl Alcohol>24 Hrs
 Methyl Butyl Ketone>24 Hrs
 Methyl Ethyl Ketone>24 Hrs
 Methylene Chloride>24 Hrs
 Naphthalene, 1-bromo->24 Hrs
 Nitric Acid (20%)>24 Hrs
 Potassium Hydroxide - Lye (10%)>24 Hrs
 Sodium Hydroxide (10%)>24 Hrs
 Sulfuric Acid (20%)>24 Hrs
 Toluene>24 Hrs
 Turpentine>24 Hrs
 Unleaded Gasoline (87 Octane)>24 Hrs
 Vinegar>24 Hrs
 Xylene>24 Hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® FP sheet Polycarbonate
Covestro Makrolon® ET IR320 Polycarbonate
Covestro Makrolon® AR sheet Polycarbonate
Covestro Makrolon® ET UV510 Polycarbonate
Covestro Makrolon® ET UV110 Polycarbonate

PCOVEST0863 / 202646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.