MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Novatec Novablend® 7813 PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: White Powder

Description: Novablend® 7813 is a rigid extrusion grade PVC compound in powder form. The formulation is designed for twin screw extrusion of exterior profiles.

Applications: Novablend®7813 is used for exterior profiles.

Information supplied by the manufacturer.

PolyOne (Avient) acquired the Novatec polymer resin product line. This grade is not a part of their current product line

Key Words: Rigid PVC compound designed for twin screw extrusion
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 - 1.47 g/cc0.0517 - 0.0531 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 44.8 MPa6500 psiASTM D638
Modulus of Elasticity 2.70 GPa392 ksiASTM D638
Flexural Yield Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 2.62 GPa380 ksiASTM D790
Izod Impact, Notched 9.60 J/cm18.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall 1601 Clear 7002 Flexible PVC
Axiall 8150 Rigid PVC, Extrusion & Molding
Axiall 7140 Rigid PVC, Extrusion & Molding
Axiall 9211 Rigid PVC, Molding
Axiall MD-5009 Rigid PVC, Molding

PNV095 / 55506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.