MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec SL200B Silicon Nitride
Categories: Ceramic; Nitride

Material Notes: SL200B ceramic material was designed especially for use in the field of welding technology. SL200B is a 100 bar gas-pressure sintered silicon nitride (Si3N4) with impressive properties. It boasts decisive advantages compared to zirconium oxide or even metal: extreme hardness and flexural strength, a high level of thermal shock resistance, electrical insulation, temperature resistance, and high tensile and compressive strength make SL200B silicon nitride ceramics a material that withstands the working conditions of projection welding and ensures a significantly longer service life. For comparison: while commonly used ceramic welding pins exhibit service lives 40 times that of metal, the service life of SL200B silicon nitride ceramics is an additional five times greater than that of centering pins made from zirconium oxide.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.21 g/cc0.116 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 16501650HV
Flexural Strength 850 MPa123000 psi
Compressive Strength 3000 MPa435000 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 21.0 W/m-K146 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1300 - 1600 °C2370 - 2910 °F
 
Descriptive Properties
Ra = Arithmetic Mean Roughness Value (µm)0.05
Thermal Shock Resistance R1 (K)700

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3
3M Techical Ceramics Ekasic® S Silicon Nitride
CeramTec SL 303 Silicon Nitride, SiAION+SiC
Silicon Nitride, reaction sintered

CCERA971 / 107571

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.