MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® FR3100 TV PC/ABS Blend  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC+ABS)-Blend; flame retardant; easy flowing; Vicat/B 120 temperature = 110 °C; increased heat resistance; improved impact strength and chemical resistance; UL recognition 94 V-1 at 1.5 mm and V-0 at 2.0 mm

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62, 50% RH
Water Absorption at Saturation 0.50 %0.50 %ISO 62
Viscosity 160000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
160000 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
melt viscosity; b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Melt Flow 25.96 g/10 min
@Load 5.00 kg,
Temperature 240 °C
25.96 g/10 min
@Load 11.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.70 GPa392 ksi1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 25.0 kJ/m²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
762 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 350 V350 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 73.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
40.6 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C196 °FISO 75-1,-2
Vicat Softening Point  108 °C
@Load 5.10 kg
226 °F
@Load 11.2 lb
50°C/h; ISO 306
 110 °C
@Load 5.10 kg
230 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 5VB
@Thickness 2.00 mm
5VB
@Thickness 0.0787 in
UL 94-5V
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FInjection molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection molding; ISO 294
Injection Velocity 240 mm/sec9.45 in/secISO 294

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® FR3050 PC/ABS Blend
Covestro Bayblend® FR3010 HF PC/ABS Blend
Covestro Bayblend® FR3005 HG PC/ABS Blend
Covestro Bayblend® FR3040 PC/ABS Blend
Covestro Bayblend® FR3010 IF PC/ABS Blend

PB09677 / 150809

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.