MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cast Nylons Nycast® CV Nylon; Caprolactam/Laurinlactum Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: A copolymer of Caprolactam and Lurinlactam, NYCAST® CV was specifically developed for use in ball valve seats in the gas and oil industry. NYCAST® CV is more resilient than Type 6 nylon. Applications range from die blocks for food processing to wobbler box inserts for the primary metals industry.

Data provided by the manufacturer, Cast Nylons Limited.

The data below are average values presented for comparison purposes. Actual property values may differ.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Water Absorption 0.50 %0.50 %24 hrs; ASTM D570
Water Absorption at Saturation 4.5 %4.5 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100 - 115100 - 115ASTM D785
Hardness, Shore D 75 - 8175 - 81ASTM D2240
Tensile Strength, Ultimate 70.0 MPa10200 psiASTM D638
Elongation at Break 25 - 80 %25 - 80 %ASTM D638
Tensile Modulus 2.00 GPa290 ksiASTM D638
Flexural Yield Strength 121 MPa17500 psiASTM D790
Flexural Modulus 2.30 GPa334 ksiASTM D790
Shear Strength 56.0 MPa8120 psiASTM D732
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
 3.7
@Frequency 1000 Hz
3.7
@Frequency 1000 Hz
 3.7
@Frequency 100000 Hz
3.7
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm559 kV/inShort time; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 77.0 µm/m-°C
@Temperature 20.0 °C
42.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 226 - 238 °C439 - 460 °FASTM D789
Maximum Service Temperature, Air 99.0 °C210 °FContinuous service
 149 °C300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C399 - 430 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 166 - 204 °C331 - 399 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Nylons Nycast® 6PA-MoS2 Nylon 6
Cast Nylons Nycast® 6PA-Blue Nylon 6
Cast Nylons Nycast® 6PA-Natural Nylon 6, Food Grade
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon
Cast Nylons Nycast® Nyloil® Lubricated Nylon

PCAST6 / 27943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.