MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPH 3866 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns, and Extrusion Coating
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Process Stability TOTAL Petrochemicals Polypropylene 3866 features excellent processability and gas fade resistance.

FDA. 3866 complies with all applicable FDA regulations for food contact applications

Recommended Applications. 3866 is recommended for spunbond nonwoven fabric high speed melt spinning applications, multifilament yarns, and extrusion coating.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccASTM D1505
Melt Flow 35 g/10 min35 g/10 minASTM D1238, L
 
Mechanical PropertiesMetricEnglishComments
Elongation at Yield 150 %150 %ASTM D3218
Tenacity 0.185 N/tex2.10 g/denierASTM D3218
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FDSC
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 250 °C399 - 482 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 3462 Polypropylene, Extrusion Grade
Braskem H 301 Injection Molding Polypropylene
Total PPH 4030 Polypropylene Homopolymer
Total PPH 3764 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics and Multifilament Yarns
Total PPH 3962 Polypropylene Homopolymer, Ultra-High Melt Flow Rate Pelletized For Melt Blown Fiber Applications

PTOTAL818 / 130543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.