MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

IRPC Polimaxx Porene SR101 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Applications:
  • extrusion sheet
  • refrigerator door liners and inner box liners
  • picnic coolers
  • snow boats
  • luggage cases

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105
@Thickness 6.35 mm,
Temperature 23.0 °C
105
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D785
Tensile Strength, Ultimate 43.1 MPa
@Temperature 23.0 °C
6260 psi
@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 59.3 MPa
@Temperature 23.0 °C
8610 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus 2.01 GPa
@Temperature 23.0 °C
292 ksi
@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 2.94 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
5.51 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
@Thickness 6.35 mm
198 °F
@Thickness 0.250 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
@Thickness 6.35 mm
185 °F
@Thickness 0.250 in
ASTM D648
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.12 mm
HB
@Thickness 0.123 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 240 °C356 - 464 °F
Drying Temperature 80.0 - 90.0 °C
@Time 7200 - 18000 sec
176 - 194 °F
@Time 2.00 - 5.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon KOCETAL® UR304 Toughened Grade Acetal Resin
Lotte Advanced Materials Starex® SV-0167 ABS, Unreinforced Extrusion Grade
Ineos ABS Lustran® ABS 595CP Refrigeration and Extrusion Grade
TPI Porene® ABS-SR101 High Impact Extrusion Grade ABS Resin
TPI Porene® ABS-SP-100 Super High Impact ABS Resin

PIRPC014 / 83991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.