Product Description: ExxonMobil™ HD 5403.AS is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance. Availability: Africa & Middle East; Europe, Latin America, North America Additive: Thermal Stabilizer: Yes; Antistatic: Yes Applications: Drainage Pipes, Food Packaging, Household and Industrial chemical containers, Pharmaceutical Packaging, Thermoformed Parts, Thin Gauge Sheet Information provided by ExxonMobil Chemical |