MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Luminex ™ 970 Mac-M0990S Technical Ceramic
Categories: Ceramic

Material Notes: A high-purity porous magnesia ceramic of typical composition.

Applications:

  • Special cabling for control systems in nuclear power stations where low neutron capture is of vital importance
  • Thermal processing equipment
  • Electrical control devices in industrial plant
  • Crushable bushes for electrical insulation at high temperature

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 - 2.70 g/cc0.0795 - 0.0975 lb/in³tailorable, fired
Porosity 24 - 38 %24 - 38 %open
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 7.00 - 85.0 MPa
@Temperature 20.0 °C
1020 - 12300 psi
@Temperature 68.0 °F
3-point
Compressive Strength 12.0 - 190 MPa1740 - 27600 psitailorable
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  5.30e+6 ohm-cm
@Temperature 1000 °C
5.30e+6 ohm-cm
@Temperature 1830 °F
 2.80e+7 ohm-cm
@Temperature 900 °C
2.80e+7 ohm-cm
@Temperature 1650 °F
 2.00e+8 ohm-cm
@Temperature 800 °C
2.00e+8 ohm-cm
@Temperature 1470 °F
 2.10e+9 ohm-cm
@Temperature 700 °C
2.10e+9 ohm-cm
@Temperature 1290 °F
 3.80e+10 ohm-cm
@Temperature 600 °C
3.80e+10 ohm-cm
@Temperature 1110 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.3 µm/m-°C
@Temperature 200 - 500 °C
7.94 µin/in-°F
@Temperature 392 - 932 °F
 14.8 µm/m-°C
@Temperature 20.0 - 1000 °C
8.22 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 8.00 - 32.0 W/m-K
@Temperature 20.0 - 900 °C
55.5 - 222 BTU-in/hr-ft²-°F
@Temperature 68.0 - 1650 °F
Maximum Service Temperature, Air 1200 °C2190 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.23 %0.23 %
CaO 0.65 %0.65 %
Fe2O3 <= 0.050 %<= 0.050 %
MgO 99 %99 %
Other >= 0.0010 %>= 0.0010 %B+Cd
SiO2 0.12 %0.12 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphorous, P, Black
Elkem (Bluestar Silicones) BLUESIL™ GUM 751 Silicone Gum
CHT Group SMP™ EP 3001 EPI Engineered Polymers Silicone Modified Polymer

CMORF8061 / 203538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.