MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Wacker® TPD Silicone Release Agent
Categories: Fluid; Polymer; Thermoset; Silicone

Material Notes: Product description: WACKER® TPD is a 100 % aminofunctional polydimethylsiloxane for the formulation of release agents for polyurethane processing.

Application: WACKER® TPD has excellent release properties and, when handled properly, prevents release agent buildup on the mould. WACKER® TPD demonstrates advantages in cases where the moldings must display a very smooth and shiny surface.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³DIN 51757
Kinematic Viscosity 300 cSt300 cSt
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.40351.4035
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearanceclear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Wacker® Catalyst EM 440 Release Coating-Silicone Emulsion
Wacker Wacker® Catalyst C 05 Release Coating
Wacker Vinnol® H 40/60 Vinyl Chloride Copolymer
Shin-Etsu Silicones KE-347T Silicone, RTV Coating
Dow SYL-OFF® PMCPSL 9112 Coating

PWACK9825 / 205354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.