MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Butvar® B-72 Polyvinyl Butyral Resin
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Product Description: Butvar® B-72 is a thermoplastic, polyvinyl butyral resin which offers a unique combination of properties for coating or adhesive applications. The use or addition of polyvinyl butyral to a system imparts adhesion, toughness, and flexibility. PVB retains the clarity of the coating and offers reactive hydroxyl sites for crosslinking with thermoset systems.

Application/Uses:

  • Binders and structural adhesives
  • Coatings for wood or metal substrates
  • Structural composites and laminates

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Volatiles <= 3.5 %<= 3.5 %
Viscosity 170 - 260 cP170 - 260 cP
Molecular Weight 170000 - 250000 g/mol170000 - 250000 g/mol
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 72.0 - 78.0 °C162 - 172 °F
 
Descriptive Properties
AppearanceWhite, free-flowing powder
Content<2.5 %Acetate Content
 17.5-20 %Hydroxyl Content
 80%Butyryl Content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Vanceva® Polyvinyl Butyral Interlayer
Beryllium, Be
Eastman Butvar® B-98 Polyvinyl Butyral Resin
Eastman Saflex® Light Neutral Brown 0.38 mm Colored Protective Interlayer PVB Film for Glass Laminates
Eastman Saflex® Light Bronze 0.38 mm Colored Protective Interlayer PVB Film for Glass Laminates

PEATM5087 / 222281

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.