MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 303-6RA11 Billet
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Sandvik 6RA11 is an austenitic chromium-nickel steel.

Information provided by Sandvik

ASTM 303; UNS S30300; EN 10088-3

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170170
Tensile Strength, Ultimate 515 - 690 MPa74700 - 100000 psi
Tensile Strength, Yield  >= 205 MPa
@Strain 0.2 %
>= 29700 psi
@Strain 0.2 %
 >= 240 MPa
@Strain 1 %
>= 34800 psi
@Strain 1 %
Elongation at Break >= 35 %>= 35 %
Reduction of Area >= 50 %>= 50 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.050 %0.050 %
Chromium, Cr 18 %18 %
Iron, Fe 70.4 %70.4 %As Balance
Manganese, Mn 1.8 %1.8 %
Nickel, Ni 9.0 %9.0 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si 0.40 %0.40 %
Sulfur, S 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
China Tungsten YG6A Tungsten Carbide for Cutting Tools
ASTM A242 Steel, type 1, 19 mm thick
China Tungsten ZK20 Tungsten Carbide
Iron, Fe
303 Stainless Steel, annealed

NSANDV147 / 19041

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.