MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil AXO3BE3 Polypropylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt flow rate and excellent processing attributes.

Availability: North America

Features:

  • Fast Molding Cycle
  • Good Flow
  • Good Stiffness
  • Impact Modified
  • Nucleated
Uses:
  • Appliances
  • Automotive Applications
  • Automotive Interior Parts
  • Compounding
  • Consumer Applications
  • Industrial Applications
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.2 MPa3650 psi2.0 in/min; ASTM D638
Elongation at Yield 4.7 %4.7 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1350 MPa196000 psi0.05 in/min; ASTM D790A
 1530 MPa222000 psi0.5 in/min; ASTM D790B
Izod Impact, Notched 0.854 J/cm1.60 ft-lb/inASTM D256A
Gardner Impact 21.5 J
@Thickness 3.17 mm,
Temperature -28.9 °C
15.8 ft-lb
@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C227 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil AXO3BE3 Impact Copolymer
ExxonMobil Exceed™ PP7815E1 Polypropylene Homopolymer
ExxonMobil AP03B Polypropylene Impact Copolymer
ExxonMobil PP1105E1 Homopolymer
ExxonMobil Achieve™ 6936G2 Polypropylene Homopolymer

PEX99404 / 175640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.