MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Maxxam™ FR PP FR 7A11 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.928 g/cc0.928 g/ccASTM D792
Melt Flow 4.6 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.6 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.3 MPa4100 psiType I, 51 mm/min; ASTM D638
Elongation at Break 200 %200 %Type I, 51 mm/min; ASTM D638
Flexural Modulus 1.24 GPa180 ksiASTM D790
Izod Impact, Notched 0.640 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.20 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
@Thickness 3.18 mm
194 °F
@Thickness 0.125 in
Unannealed; ASTM D648
UL RTI, Electrical  105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
UL 746
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
UL 746
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
UL 746
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-2
@Thickness 0.794 mm
V-2
@Thickness 0.0313 in
ALL; UL 94
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
UL 94
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
UL 94
 
Descriptive Properties
FeaturesFlame Retardant
 Medium Flow
 Medium Impact Resistance
FormsPellets
Generic MaterialPP, Unspecified
Generic NamePolypropylene, Unspecified (PP, Unspecified)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam™ FR PE 161-1A Polyethylene, High Density (HDPE)
Avient Maxxam™ FR PP 301 EXT Polypropylene
Avient Maxxam™ FR PP 401 Polypropylene
Overview of materials for Polypropylene, Flame Retardant
Avient Maxxam™ FR PP 301 S Polypropylene

PH0POL0164 / 144733

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.