System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Wellman Wellamid® GS40-66 22L-N 40% Glass Sphere Filled Nylon 66, Lubricated
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Glass Bead Filled
Material Notes:
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.
Data provided by the manufacturer, Wellman Inc.
Key Words:
Polyamide 66
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.44
g/cc
0.0520
lb/in³
ISO 1183
Water Absorption
1.2 %
1.2 %
Approximate 24 hr.
Linear Mold Shrinkage
0.010
-
0.014
cm/cm
0.010
-
0.014
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
75.0
MPa
10900
psi
ISO 527
Elongation at Break
3.0 %
3.0 %
ISO 527
Flexural Yield Strength
125
MPa
18100
psi
ISO 178
Flexural Modulus
5.00
GPa
725
ksi
ISO 178
Izod Impact, Notched
0.300
J/cm
0.562
ft-lb/in
ISO 180
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
105
°C
221
°F
ISO 75
Flammability, UL94
HB
@Thickness 1.57 mm
HB
@Thickness 0.0618 in
UL 94
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
282
-
304
°C
540
-
580
°F
Middle Barrel Temperature
271
-
288
°C
520
-
550
°F
Front Barrel Temperature
260
-
277
°C
500
-
530
°F
Nozzle Temperature
260
-
288
°C
500
-
550
°F
Melt Temperature
277
-
304
°C
530
-
580
°F
Mold Temperature
71.1
-
93.3
°C
160
-
200
°F
Drying Temperature
79.4
°C
175
°F
Opened bags and gaylord boxes
Dry Time
2
-
4
hour
2
-
4
hour
Opened bags and gaylord boxes
Moisture Content
0.050 - 0.20 %
0.050 - 0.20 %
During molding to prevent hydrolytic degradation
<= 0.20 %
<= 0.20 %
In shipping bags, ready to mold
Injection Pressure
34.5
-
138
MPa
5000
-
20000
psi
Back Pressure
0.345
MPa
50.0
psi
Screw Speed
60
-
120
rpm
60
-
120
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celanex® J600 PBT, 40% Mineral / Glass Reinforced
Wellman Wellamid® GSF1849-N1 Nylon 66, 40% Glass Sphere/Fiber Reinforced
Wellman Wellamid® GS40-60 42L-N 40% Glass Sphere Filled Nylon 6, Lubricated
PWEL33 / 72313
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.