MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes:

Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Melt Flow 8.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
8.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength 37.9 MPa
@Thickness 3.17 mm
5500 psi
@Thickness 0.125 in
ASTM D638
Flexural Strength 65.5 MPa
@Thickness 3.17 mm
9500 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.24 GPa
@Thickness 3.17 mm
325 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched  1.44 J/cm
@Thickness 6.35 mm
2.70 ft-lb/in
@Thickness 0.250 in
ASTM D256
 1.60 J/cm
@Thickness 3.17 mm
3.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.3 °C182 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C170 °FASTM D648
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL file E155285
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 182 °C340 - 360 °F
Middle Barrel Temperature 199 - 210 °C390 - 410 °F
Front Barrel Temperature 204 - 216 °C400 - 420 °F
Nozzle Temperature 204 - 216 °C400 - 420 °F
Melt Temperature 193 - 232 °C380 - 450 °F
Mold Temperature 54.4 - 71.1 °C130 - 160 °F
Drying Temperature 87.8 °C190 °Fmax 6 hours
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 55.2 - 82.7 MPa8000 - 12000 psi
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Shot Size 50 - 80 %50 - 80 %
Vent Depth 0.00381 - 0.00762 cm0.00150 - 0.00300 in
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant
Aclo Accucomp ABS ABS802L High Impact Grade
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Medium Density Polyethylene (MDPE), Molded

PZ9PT00n / 178345

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.