Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520. Applications Benefits- Low gloss
- High impact resistance
|