MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 155 A Polypropylene (PP) Mineral - Flame Retardant - Non-PBB/PBDE - UL94 V-0
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D 792
Water Absorption 0.030 %
@Time 86400 sec
0.030 %
@Time 24.0 hour
ASTM D 570
Additive Loading 20 %20 %Primary Additive
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
@Thickness 3.20 mm
0.0070 - 0.010 in/in
@Thickness 0.126 in
ASTM D 955
Melt Flow 4.0 - 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 - 6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.7 MPa3000 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 2.21 GPa320 ksiASTM D 638
Flexural Strength 37.9 MPa5500 psiASTM D 790
Flexural Modulus 2.41 GPa350 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 6.41 J/cm
@Thickness 3.20 mm
12.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C257 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FASTM D 648
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 - 232 °C375 - 450 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 300 TFE 10 SE Polycarbonate (PC), Unreinforced - PTFE Lubricated - Self Extinguishing - Bromine/Chlorine Free - UL94 V-1
RTP Company RTP 104 CC FR A UV Polypropylene (PP), Glass Fiber - Chemically Coupled - Flame Retardant - Non- PBB/PBDE - UV Stabilized
RTP Company RTP 199 X 124807 Polypropylene (PP) Flame Retardant - UV Stabilized
RTP Company RTP 128 FR Polypropylene (PP), Talc - Flame Retardant
RTP Company RTP 103 FR A Polypropylene (PP), Glass Fiber - Flame Retardant - Non-PBB/PBDE

PQZTA14182 / 171728

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.