MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Resin Type: VA Copolymer

Characteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strength

Applications:Laminations, Heavy produce and skin packaging, Frozen food packaging

Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.

Film properties below based on film thickness of 31.8 µm.

Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.929 g/cc0.0336 lb/in³ASTM D1505
Melt Flow 1.3 g/10 min1.3 g/10 minCondition E; ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Secant Modulus, MD 0.150 GPa21.8 ksiASTM D882
Secant Modulus, TD 0.170 GPa24.7 ksiASTM D882
Coefficient of Friction 0.400.40ASTM D1894
Dart Drop 3.90 g/micron99.1 g/milF50; 1.5 in. dart/26 in. drop height; ASTM D 1709
 
Optical PropertiesMetricEnglishComments
Haze 5.5 %5.5 %ASTM D2457
Gloss 69 %69 %at 45°. ASTM D 2457
 110 %110 %at 60°. ASTM D 2457
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 °C399 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvax® 440 Ethylene Vinyl Acetate
Dow Elvax® 40L-03 Ethylene-Vinyl Acetate Copolymer Resin
Dow Elvax® 3120 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA)
Bostik 140 Low Cost EVA Glue Stick

PCHEVV92 / 20488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.