MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 - 2.10 g/cc0.0592 - 0.0759 lb/in³Average value: 1.85 g/cc Grade Count:45
Water Absorption 0.130 - 0.350 %0.130 - 0.350 %Average value: 0.245 % Grade Count:37
 0.250 - 0.250 %
@Temperature 50.0 - 50.0 °C
0.250 - 0.250 %
@Temperature 122 - 122 °F
Average value: 0.250 % Grade Count:4
 0.250 - 0.250 %
@Time 173000 - 173000 sec
0.250 - 0.250 %
@Time 48.0 - 48.0 hour
Average value: 0.250 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm0.00100 - 0.00600 in/inAverage value: 0.00291 cm/cm Grade Count:45
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 35.0 - 689 MPa5080 - 100000 psiAverage value: 75.7 MPa Grade Count:36
Tensile Strength, Yield 30.0 - 100 MPa4350 - 14500 psiAverage value: 69.6 MPa Grade Count:5
Modulus of Elasticity 4.00 - 17.0 GPa580 - 2470 ksiAverage value: 9.55 GPa Grade Count:8
Flexural Yield Strength 60.0 - 180 MPa8700 - 26100 psiAverage value: 118 MPa Grade Count:45
Flexural Modulus 8.00 - 18.0 GPa1160 - 2610 ksiAverage value: 12.9 GPa Grade Count:33
Compressive Yield Strength 130 - 200 MPa18900 - 29000 psiAverage value: 163 MPa Grade Count:42
Izod Impact, Notched 0.267 - 2.40 J/cm0.500 - 4.50 ft-lb/inAverage value: 0.616 J/cm Grade Count:33
Charpy Impact Unnotched 0.200 - 1.50 J/cm²0.952 - 7.14 ft-lb/in²Average value: 0.730 J/cm² Grade Count:9
Charpy Impact, Notched 0.120 - 0.800 J/cm²0.571 - 3.81 ft-lb/in²Average value: 0.371 J/cm² Grade Count:11
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+17 ohm-cm1.00e+14 - 1.00e+17 ohm-cmAverage value: 3.92e+16 ohm-cm Grade Count:19
 1.00e+10 - 1.00e+10 ohm-cm
@Temperature 70.0 - 70.0 °C
1.00e+10 - 1.00e+10 ohm-cm
@Temperature 158 - 158 °F
Average value: 1.00e+10 ohm-cm Grade Count:4
 1.00e+10 - 1.00e+10 ohm-cm
@Time 2.59e+6 - 2.59e+6 sec
1.00e+10 - 1.00e+10 ohm-cm
@Time 720 - 720 hour
Average value: 1.00e+10 ohm-cm Grade Count:4
Surface Resistance 1.00e+14 - 1.00e+17 ohm1.00e+14 - 1.00e+17 ohmAverage value: 3.72e+16 ohm Grade Count:20
 1.00e+10 - 1.00e+10 ohm
@Temperature 70.0 - 70.0 °C
1.00e+10 - 1.00e+10 ohm
@Temperature 158 - 158 °F
Average value: 1.00e+10 ohm Grade Count:4
 1.00e+10 - 1.00e+10 ohm
@Time 2.59e+6 - 2.59e+6 sec
1.00e+10 - 1.00e+10 ohm
@Time 720 - 720 hour
Average value: 1.00e+10 ohm Grade Count:4
Insulation Resistance 1.00e+14 - 1.00e+15 ohm1.00e+14 - 1.00e+15 ohmAverage value: 4.83e+14 ohm Grade Count:3
Dielectric Constant 3.50 - 5.503.50 - 5.50Average value: 4.12 Grade Count:41
Dielectric Strength 12.0 - 40.0 kV/mm305 - 1020 kV/inAverage value: 15.5 kV/mm Grade Count:44
Dielectric Breakdown 60.0 - 64.0 V60.0 - 64.0 VAverage value: 61.5 V Grade Count:4
Dissipation Factor 0.00500 - 0.03000.00500 - 0.0300Average value: 0.0145 Grade Count:41
Arc Resistance 130 - 240 sec130 - 240 secAverage value: 151 sec Grade Count:35
Track Resistance 600 sec600 secAverage value: 600 sec Grade Count:6
Comparative Tracking Index 500 - 600 V500 - 600 VAverage value: 582 V Grade Count:25
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 - 55.0 µm/m-°C6.67 - 30.6 µin/in-°FAverage value: 20.2 µm/m-°C Grade Count:32
 5.00 - 60.0 µm/m-°C
@Temperature 50.0 - 100 °C
2.78 - 33.3 µin/in-°F
@Temperature 122 - 212 °F
Average value: 31.3 µm/m-°C Grade Count:8
Thermal Conductivity 0.280 - 1.10 W/m-K1.94 - 7.63 BTU-in/hr-ft²-°FAverage value: 0.482 W/m-K Grade Count:20
Maximum Service Temperature, Air 130 - 180 °C266 - 356 °FAverage value: 138 °C Grade Count:17
Deflection Temperature at 1.8 MPa (264 psi) 180 - 295 °C356 - 563 °FAverage value: 241 °C Grade Count:39
Deflection Temperature at 8.0 MPa 120 - 200 °C248 - 392 °FAverage value: 165 °C Grade Count:8
Heat Distortion Temperature 260 °C500 °FAverage value: 260 °C Grade Count:4
Flammability, UL94 HB - V-0HB - V-0Grade Count:25
Oxygen Index 21.0 - 50.0 %21.0 - 50.0 %Average value: 35.2 % Grade Count:19
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 180 °C275 - 356 °FAverage value: 159 °C Grade Count:14
Mold Temperature 135 - 190 °C275 - 374 °FAverage value: 162 °C Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
G-10 Fiberglass Epoxy Laminate Sheet
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets

O1530 / 77880

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.