MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

General Plastics LAST-A-FOAM® FR-10110 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.160 g/cc0.00578 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.49 MPa216 psiParallel to Rise; ASTM D1623
 1.50 MPa218 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 2.34 MPa340 psiRise Parallel to Test Span; ASTM D790
 2.36 MPa343 psiRise Parallel to Beam Thick.; ASTM D790
Flexural Modulus 0.11110 GPa16.114 ksiRise Parallel to Test Span; ASTM D790
 0.11643 GPa16.887 ksiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength  1.53 MPa
@Temperature 177 °C
222 psi
@Temperature 350 °F
Parallel to Rise; ASTM D1621
 1.88 MPa
@Temperature 177 °C
273 psi
@Temperature 350 °F
Perpendicular to Rise; ASTM D1621
 2.34 MPa
@Temperature 121 °C
339 psi
@Temperature 250 °F
Parallel to Rise; ASTM D1621
 2.48 MPa
@Temperature 121 °C
359 psi
@Temperature 250 °F
Perpendicular to Rise; ASTM D1621
 3.24 MPa
@Temperature 23.9 °C
470 psi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 3.33 MPa
@Temperature 23.9 °C
483 psi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
Compressive Modulus  0.03995 GPa
@Temperature 177 °C
5.794 ksi
@Temperature 350 °F
Parallel to Rise; ASTM D1621
 0.04704 GPa
@Temperature 177 °C
6.823 ksi
@Temperature 350 °F
Perpendicular to Rise; ASTM D1621
 0.0570 GPa
@Temperature 121 °C
8.26 ksi
@Temperature 250 °F
Parallel to Rise; ASTM D1621
 0.05719 GPa
@Temperature 121 °C
8.294 ksi
@Temperature 250 °F
Perpendicular to Rise; ASTM D1621
 0.073457 GPa
@Temperature 23.9 °C
10.654 ksi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
 0.07433 GPa
@Temperature 23.9 °C
10.78 ksi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
Poissons Ratio 0.300.30
 
Thermal PropertiesMetricEnglishComments
CTE, linear 37.8 µm/m-°C
@Temperature -28.9 - 71.1 °C
21.0 µin/in-°F
@Temperature -20.0 - 160 °F
GP Method
Thermal Conductivity 0.0389 W/m-K0.270 BTU-in/hr-ft²-°FASTM C518
 
Descriptive Properties
Tumbling Friability (%)2620 mins at 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-10108 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-10106 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3830 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3818 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3808 FST Polyurethane Foam

PGENR060 / 186846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.