MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom G3 U01 R NAT Polypropylene with 30% Glass Fiber Filler  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Hostacom G3 U01 R NAT is a 30% glass fiber reinforced PP homopolymer, with good flowability and high rigidity. The product is only available as natural, pellet form. Dry material before processing. Applications: Industrial Packaging

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183-1A
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
14 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 95.0 MPa13800 psiISO 527-1,-2
Elongation at Yield 2.8 %2.8 %ISO 527-1,-2
Tensile Modulus 6.80 GPa986 ksiISO 527-1,-2
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179-1/1eU
Charpy Impact, Notched  0.750 J/cm²
@Temperature -20.0 °C
3.57 ft-lb/in²
@Temperature -4.00 °F
ISO 179-1/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FISO 75-1,-2
Vicat Softening Point 135 °C275 °FB50N; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom G3 U01 102297 Polypropylene with 30% Glass Fiber Filler
LyondellBasell Hostacom G3 N01 102297 Polypropylene with 30% Glass Fiber Filler
LyondellBasell Hostacom G3 N01 L Polypropylene with 30% Glass Fiber Filler
Avient Maxxam™ FR 8000 Polypropylene with 30% Glass Fiber
LyondellBasell Hostacom G3 R05 105555 Polypropylene with 30% Glass Fiber Filler

PEQT7948 / 219585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.