MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil PP8013L1 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, tools and boxes. It is also suitable as compound base stock applications.

Availability: Africa & Middle East and Europe

Features:

  • Ductile
  • Medium Flow
  • Nucleated
  • Ultra High Impact Resistance
Uses:
  • Compounding
  • Construction Applications
  • Industrial Applications
  • Rigid Packaging
Processing Method: Injection Molding and Compounding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ISO 868
Tensile Strength, Yield 17.0 MPa2470 psiISO 527-2/50
Elongation at Yield 4.0 %4.0 %ISO 527-2/50
Tensile Modulus 0.951 GPa138 ksiISO527-2/1
Flexural Modulus 0.903 GPa131 ksiISO 178
Izod Impact, Notched (ISO) 50.4 kJ/m²24.0 ft-lb/in²ISO 180/1A
Charpy Impact, Notched  1.01 J/cm²
@Temperature -20.0 °C
4.80 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 1.41 J/cm²
@Temperature 0.000 °C
6.70 ft-lb/in²
@Temperature 32.0 °F
ISO 179/1eA
 4.41 J/cm²
@Temperature 22.8 °C
21.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 163 °C325 °FISO 3146
Crystallization Temperature 256 °C493 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 46.1 °C115 °FISO 75-2/A
Vicat Softening Point 140 °C284 °FISO 306/A50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil PP7011L1 Polypropylene Impact Copolymer
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
ExxonMobil PP7033L1 Polypropylene Impact Copolymer
ExxonMobil PP7043L1 Polypropylene Impact Copolymer
ExxonMobil PP7032E2 Impact Copolymer

PEX99432 / 175668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.