MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Crastin® FGS600F40 NC010 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Melt Density 1.11 g/cc
@Temperature 250 °C
0.0401 lb/in³
@Temperature 482 °F
Water Absorption 0.40 %
@Thickness 2.00 mm
0.40 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.016 cm/cm0.016 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4, 2577
Melt Flow 37 g/10 min
@Load 2.16 kg,
Temperature 250 °C
37 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psiISO 527-1/-2
Elongation at Break 30 %30 %Nominal; ISO 527-1/-2
Elongation at Yield 4.0 %4.0 %ISO 527-1/-2
Tensile Modulus 2.40 GPa348 ksiISO 527-1/-2
Poissons Ratio 0.380.38
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2600 MPa377000 psi1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 1800 MPa261000 psi1000h; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 62631-3-2
Dielectric Strength 26.0 kV/mm660 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 62631-2-1
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 2.11 J/g-°C
@Temperature 250 °C
0.504 BTU/lb-°F
@Temperature 482 °F
Melt
Thermal Conductivity 0.210 W/m-K
@Temperature 250 °C
1.46 BTU-in/hr-ft²-°F
@Temperature 482 °F
Melt
Melting Point 223 °C433 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FISO 75-1/-2
 180 °C356 °FAnnealed; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
 60.0 °C140 °FAnnealed; ISO 75-1/-2
Vicat Softening Point 175 °C347 °F50°C/h, 50N; ISO 306
Glass Transition Temp, Tg 55.0 °C131 °F10°C/min; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
IEC 60695-11-10
Flame Spread 28.0 mm/min
@Thickness 1.00 mm
1.10 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 22 %22 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FOptimum, Injection
 240 - 260 °C464 - 500 °FRange, Injection
Mold Temperature 80.0 °C176 °FOptimum, Injection
 30.0 - 130 °C86.0 - 266 °FInjection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.040 %<= 0.040 %Injection
Hold Pressure >= 60.0 MPa>= 8700 psiInjection
 
Descriptive Properties
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (%)95F-value (refraction); ISO 6452
Fogging (mg)0.2G-value (condensate); ISO 6452
Odor Class3VDA 270
Part Marking Code>PBT<ISO 11469
PolymerPBT
Processing Hold Pressure Time (s/mm)4Injection
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPBTISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Crastin® FGS600F10 NC010 PBT
DuPont Mobility and Materials Crastin® FG6129 NC010 PBT
Arkema Pebax® 4533 SP 01 TPA
Celanese Crastin® S600F20 NC010 PBT
Celanese Crastin® S610SF NC010 PBT

PDSX5015 / 197655

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.