MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 100 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and thermal stability. These films are known for good roll formation and consistency of quality.

The following Teijin® Tetoron® S film variants are available:
S: Non-pretreated
SG: Low thermal shrinkage
SG2: Low thermal shrinkage; Adhesion Pretreated (one side)
SGZ: Release Liner (one side)
SD: Adhesion Pretreated (one side)
SP: Adhesion Pretreated (one side)
SDW: Adhesion Pretreated (two side)
SEW: Adhesion Pretreated (two side)
PS: Sand blasted S film (matte)

Typical Applications:

  • Printing Plates
  • Tracing
  • Flexible Printed Circuits (FPC)
  • Membrane Touch Switch (MTS)

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 140 %140 %ASTM D882A
Film Elongation at Break, TD 120 %120 %ASTM D882A
Coefficient of Friction, Dynamic 0.410.41ASTM D1894
Coefficient of Friction, Static 0.400.40ASTM D1894
Film Tensile Strength at Break, MD 254.93 MPa36975 psiASTM D882A
Film Tensile Strength at Break, TD 293.9 MPa42630 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 1.3 %
@Temperature 150 °C,
Time 1800 sec
1.3 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.30 %
@Temperature 150 °C,
Time 1800 sec
0.30 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Teijin® Tetoron® OLF Polyester Film, 700 Gauge
DuPont Teijin Films Teijin® Tetoron® O Polyester Film, 300 Gauge
DuPont Teijin Films Teijin® Tetoron® SLA Polyester Film, 200 Gauge
DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 200 Gauge
DuPont Teijin Films Teijin® Tetoron® OX Polyester Film, 200 Gauge

PDTZ9469 / 139786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.