MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Vistalon™ 6505 Ethylene Propylene Diene Terpolymer Rubber  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Description: Vistalon 6505 EPDM rubber is a medium Mooney polymer with low ethylene and high diene content. It has a medium molecular weight distribution. It is applicable for extruded seals and gaskets. This product is sold in dense bales.

Key Features:

  • Designed for extrusion applications.
  • Fast cure and high cure state

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 53
@Temperature 125 °C
53
@Temperature 257 °F
ML(1+4), Radial cavity dies, polymer remassed at 145±°C; ASTM D1646
 
Descriptive Properties
Ethylene Content57.0 wt%ASTM D3900
Ethylidenenorbornene (ENB) Content9.2 wt%ASTM D6047

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Monarch® F-03092 (Black) EPDM Foam
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
Armacell Ensolite™ EF0 EPDM crushed foam
ExxonMobil Vistalon™ 3702 Ethylene Propylene Diene Terpolymer Rubber
ExxonMobil Vistalon™ 7800 Bimodal EPDM Polymer

PEXA930 / 125973

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.