MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMODUR® LU-T80 + BAYTEC® XL 2190 Polyurethane, TDI-PTMEG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccDESMODUR® LU-T80
 1.24 g/cc1.24 g/ccBAYTEC® XL 2190
Viscosity 600 cP600 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090DIN 53505
 91
@Temperature 80.0 °C
91
@Temperature 176 °F
DIN 53505
 92
@Temperature -5.00 °C
92
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 34.0 MPa4930 psiDIN 53504
Tensile Stress at Strain 3.60 MPa
@Strain 10 %
522 psi
@Strain 10 %
DIN 53504
Elongation at Break 475 %475 %DIN 53504
100% Modulus 8.40 MPa
@Strain 100 %
1220 psi
@Strain 100 %
DIN 53504
200% Modulus 10.4 MPa
@Strain 200 %
1510 psi
@Strain 200 %
DIN 53504
300% Modulus 13.1 MPa
@Strain 300 %
1900 psi
@Strain 300 %
DIN 53504
Resilience 5858[%]; DIN 53512
Tear Strength 28.0 kN/m160 pliwith nick; ISO 34-1
 102 kN/m582 pliwithout nick; ISO 34-1
Abrasion 5050[mm3]; ISO 4649
Compression Set  23 %
@Temperature 25.0 °C,
Time 259000 sec
23 %
@Temperature 77.0 °F,
Time 72.0 hour
ISO 815-1
 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FDESMODUR® LU-T80
 110 °C230 °FBAYTEC® XL 2190
Mold Temperature 100 °C212 °F
Pot Life 5.75 min5.75 min
 
Descriptive Properties
AppearancesolidDESMODUR® LU-T80
 solidBAYTEC® XL 2190
Content100Parts by weight of prepolymer
 13.75Parts by weight of BAYTEC® XL 2190
 3--3.4%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® LU-D80 + MOCA Polyurethane, TDI-Ester
Covestro DESMODUR® LU-T80 + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Covestro DESMODUR® LU-T60D + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Covestro DESMODUR® LU-T70D + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Covestro DESMODUR® LU-T75D + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG

PCOVEST0378 / 202161

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.