MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.63 g/cc0.0434 - 0.0589 lb/in³Average value: 1.33 g/cc Grade Count:164
Filler Content 5.00 - 40.0 %5.00 - 40.0 %Average value: 19.9 % Grade Count:53
Water Absorption 0.0500 - 0.900 %0.0500 - 0.900 %Average value: 0.130 % Grade Count:58
Moisture Absorption at Equilibrium 0.100 - 0.250 %0.100 - 0.250 %Average value: 0.163 % Grade Count:11
Water Absorption at Saturation 0.120 - 0.350 %0.120 - 0.350 %Average value: 0.235 % Grade Count:9
Additive Loading 10.0 - 30.0 %10.0 - 30.0 %Average value: 18.0 % Grade Count:10
Maximum Moisture Content 0.02000.0200Average value: 0.0200 Grade Count:7
Linear Mold Shrinkage 0.000200 - 0.00900 cm/cm0.000200 - 0.00900 in/inAverage value: 0.00336 cm/cm Grade Count:143
Linear Mold Shrinkage, Transverse 0.00200 - 0.00750 cm/cm0.00200 - 0.00750 in/inAverage value: 0.00460 cm/cm Grade Count:27
Melt Flow 3.00 - 22.0 g/10 min3.00 - 22.0 g/10 minAverage value: 10.3 g/10 min Grade Count:57
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 83.0 - 95.083.0 - 95.0Average value: 85.7 Grade Count:9
Hardness, Rockwell R 81.0 - 12481.0 - 124Average value: 119 Grade Count:43
Tensile Strength, Ultimate 45.0 - 172 MPa6530 - 24900 psiAverage value: 87.0 MPa Grade Count:125
 25.0 - 85.0 MPa
@Temperature 60.0 - 120 °C
3630 - 12300 psi
@Temperature 140 - 248 °F
Average value: 60.0 MPa Grade Count:2
Tensile Strength, Yield 45.0 - 172 MPa6530 - 24900 psiAverage value: 78.5 MPa Grade Count:61
Elongation at Break 1.00 - 100 %1.00 - 100 %Average value: 8.82 % Grade Count:140
 1.50 - 28.0 %
@Temperature 60.0 - 120 °C
1.50 - 28.0 %
@Temperature 140 - 248 °F
Average value: 38.8 % Grade Count:2
Elongation at Yield 4.00 - 14.0 %4.00 - 14.0 %Average value: 6.73 % Grade Count:11
 2.20 - 3.00 %
@Temperature 60.0 - 120 °C
2.20 - 3.00 %
@Temperature 140 - 248 °F
Average value: 2.67 % Grade Count:1
Modulus of Elasticity 2.20 - 16.5 GPa319 - 2390 ksiAverage value: 5.73 GPa Grade Count:71
 2.20 - 6.00 GPa
@Temperature 60.0 - 120 °C
319 - 870 ksi
@Temperature 140 - 248 °F
Average value: 4.02 GPa Grade Count:2
Flexural Yield Strength 52.0 - 262 MPa7540 - 38000 psiAverage value: 132 MPa Grade Count:140
Flexural Modulus 2.40 - 12.4 GPa348 - 1800 ksiAverage value: 4.95 GPa Grade Count:158
Compressive Yield Strength 96.5 - 148 MPa14000 - 21500 psiAverage value: 114 MPa Grade Count:3
Izod Impact, Notched 0.427 - 8.00 J/cm0.800 - 15.0 ft-lb/inAverage value: 1.31 J/cm Grade Count:133
 1.00 - 1.20 J/cm
@Temperature -20.0 - 0.000 °C
1.87 - 2.25 ft-lb/in
@Temperature -4.00 - 32.0 °F
Average value: 0.996 J/cm Grade Count:4
 0.900 - 1.08 J/cm
@Temperature -30.0 - -30.0 °C
1.69 - 2.02 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 0.996 J/cm Grade Count:4
 0.900 - 1.08 J/cm
@Thickness 3.20 - 3.20 mm
1.69 - 2.02 ft-lb/in
@Thickness 0.126 - 0.126 in
Average value: 0.996 J/cm Grade Count:4
Izod Impact, Unnotched 0.400 J/cm - NB0.749 ft-lb/in - NBAverage value: 9.24 J/cm Grade Count:43
Izod Impact, Notched (ISO) 7.00 - 11.0 kJ/m²3.33 - 5.23 ft-lb/in²Average value: 8.75 kJ/m² Grade Count:12
Charpy Impact Unnotched 3.50 J/cm² - NB16.7 ft-lb/in² - NBAverage value: 5.66 J/cm² Grade Count:14
 0.800 J/cm² - NB
@Temperature -30.0 - -20.0 °C
3.81 ft-lb/in² - NB
@Temperature -22.0 - -4.00 °F
Average value: 3.50 J/cm² Grade Count:5
Charpy Impact, Notched 0.600 - 2.00 J/cm²2.86 - 9.52 ft-lb/in²Average value: 0.998 J/cm² Grade Count:23
 0.600 - 0.700 J/cm²
@Temperature -20.0 - -20.0 °C
2.86 - 3.33 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 0.629 J/cm² Grade Count:7
Tensile Impact Strength 53.3 - 147 kJ/m²25.4 - 69.9 ft-lb/in²Average value: 84.6 kJ/m² Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1e+05 - 4.00e+16 ohm-cm1e+05 - 4.00e+16 ohm-cmAverage value: 8.18e+15 ohm-cm Grade Count:62
Surface Resistance 1.00e+9 - 1.00e+16 ohm1.00e+9 - 1.00e+16 ohmAverage value: 2.70e+15 ohm Grade Count:21
Static Decay 2.00 sec2.00 secAverage value: 2.00 sec Grade Count:4
Dielectric Constant 3.00 - 3.803.00 - 3.80Average value: 3.30 Grade Count:27
Dielectric Strength 17.0 - 38.0 kV/mm432 - 965 kV/inAverage value: 22.7 kV/mm Grade Count:41
Dissipation Factor 0.000800 - 0.02000.000800 - 0.0200Average value: 0.00650 Grade Count:26
Arc Resistance 0.000 - 120 sec0.000 - 120 secAverage value: 96.5 sec Grade Count:15
Comparative Tracking Index 100 - 250 V100 - 250 VAverage value: 169 V Grade Count:20
Hot Wire Ignition, HWI 30.0 - 120 sec30.0 - 120 secAverage value: 76.3 sec Grade Count:7
High Amp Arc Ignition, HAI 15.0 - 120 arcs15.0 - 120 arcsAverage value: 99.4 arcs Grade Count:7
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minAverage value: 115 mm/min Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 40.0 µm/m-°C11.1 - 22.2 µin/in-°FAverage value: 29.1 µm/m-°C Grade Count:18
CTE, linear, Transverse to Flow 60.0 - 109 µm/m-°C33.3 - 60.5 µin/in-°FAverage value: 67.7 µm/m-°C Grade Count:7
Thermal Conductivity 0.216 - 0.350 W/m-K1.50 - 2.43 BTU-in/hr-ft²-°FAverage value: 0.294 W/m-K Grade Count:3
Maximum Service Temperature, Air 110 - 143 °C230 - 289 °FAverage value: 132 °C Grade Count:16
Hot Ball Pressure Test 125 - 135 °C257 - 275 °FAverage value: 133 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 115 - 265 °C239 - 509 °FAverage value: 147 °C Grade Count:105
Deflection Temperature at 1.8 MPa (264 psi) 104 - 207 °C220 - 405 °FAverage value: 139 °C Grade Count:129
Vicat Softening Point 125 - 186 °C257 - 367 °FAverage value: 149 °C Grade Count:35
Heat Distortion Temperature 140 - 146 °C284 - 295 °FAverage value: 144 °C Grade Count:4
UL RTI, Electrical 80.0 - 130 °C176 - 266 °FAverage value: 90.4 °C Grade Count:25
UL RTI, Mechanical with Impact 80.0 - 125 °C176 - 257 °FAverage value: 89.0 °C Grade Count:25
UL RTI, Mechanical without Impact 80.0 - 130 °C176 - 266 °FAverage value: 89.6 °C Grade Count:25
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:159
Oxygen Index 31.0 - 37.1 %31.0 - 37.1 %Average value: 34.8 % Grade Count:10
Glow Wire Test 825 - 960 °C1520 - 1760 °FAverage value: 939 °C Grade Count:23
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 343 °C410 - 649 °FAverage value: 278 °C Grade Count:27
Nozzle Temperature 249 - 338 °C480 - 640 °FAverage value: 300 °C Grade Count:22
Melt Temperature 221 - 343 °C430 - 649 °FAverage value: 293 °C Grade Count:91
Mold Temperature 60.0 - 130 °C140 - 266 °FAverage value: 97.6 °C Grade Count:106
Drying Temperature 80.0 - 149 °C176 - 300 °FAverage value: 117 °C Grade Count:92
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.0312 % Grade Count:34
Dew Point -40.0 - -17.8 °C-40.0 - 0.000 °FAverage value: -28.2 °C Grade Count:32
Drying Air Flow Rate 22.7 - 28.3 l/min0.800 - 1.00 ft³/min (CFM)Average value: 25.5 l/min Grade Count:4
Injection Pressure 4.96 - 138 MPa720 - 20000 psiAverage value: 85.1 MPa Grade Count:48
Vent Depth 0.00127 - 0.00762 cm0.000500 - 0.00300 inAverage value: 0.00301 cm Grade Count:15
Cushion 0.635 cm0.250 inAverage value: 0.635 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polycarbonate, 10% Glass Filled
Overview of materials for Polycarbonate, 20% Glass Filled
Overview of materials for Polycarbonate, UV Stabilized
Overview of materials for Polycarbonate, Molded

O3110 / 78129

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.